Your browser doesn't support javascript.
loading
Mechanical and in vitro degradation behavior of magnesium-bioactive glass composites prepared by SPS for biomedical applications.
Dutta, Sourav; Devi, K Bavya; Gupta, Sanjay; Kundu, Biswanath; Balla, Vamsi Krishna; Roy, Mangal.
Afiliação
  • Dutta S; Advanced Technology Development Centre, Indian Institute of Technology-Kharagpur, Kharagpur, 721302, India.
  • Devi KB; Department of Metallurgical and Materials Engineering, Indian Institute of Technology-Kharagpur, Kharagpur, 721302, India.
  • Gupta S; Department of Mechanical Engineering, Indian Institute of Technology-Kharagpur, Kharagpur, 721302, India.
  • Kundu B; Bioceramics & Coating Division, CSIR-Central Glass & Ceramics Research Institute (CGCRI), 196, Raja S.C. Mullick Road, Kolkata, 700032, India.
  • Balla VK; Bioceramics & Coating Division, CSIR-Central Glass & Ceramics Research Institute (CGCRI), 196, Raja S.C. Mullick Road, Kolkata, 700032, India.
  • Roy M; Department of Metallurgical and Materials Engineering, Indian Institute of Technology-Kharagpur, Kharagpur, 721302, India.
J Biomed Mater Res B Appl Biomater ; 107(2): 352-365, 2019 02.
Article em En | MEDLINE | ID: mdl-29656470

Texto completo: 1 Base de dados: MEDLINE Assunto principal: Teste de Materiais / Fixadores Internos / Vidro / Magnésio Limite: Humans Idioma: En Ano de publicação: 2019 Tipo de documento: Article

Texto completo: 1 Base de dados: MEDLINE Assunto principal: Teste de Materiais / Fixadores Internos / Vidro / Magnésio Limite: Humans Idioma: En Ano de publicação: 2019 Tipo de documento: Article