Direct-Contact Microelectrical Measurement of the Electrical Resistivity of a Solid Electrolyte Interface.
Park, Jun-Hyoung; Choi, Yong-Seok; Lee, Hyun-Jeong; Shim, Hyung-Cheoul; Ahn, Jae-Pyoung; Lee, Jae-Chul.
Afiliação
  • Park JH; Department of Materials Science and Engineering , Korea University , Seoul 02841 , South Korea.
  • Choi YS; Department of Materials Science and Engineering , Korea University , Seoul 02841 , South Korea.
  • Lee HJ; Department of Materials Science and Engineering , Korea University , Seoul 02841 , South Korea.
  • Shim HC; Advanced Analysis Center , Korea Institute of Science and Technology , Seoul 02792 , South Korea.
  • Ahn JP; Department of Applied Nano-Mechanics , Korea Institute of Machinery and Materials , Daejeon 34103 , South Korea.
  • Lee JC; Advanced Analysis Center , Korea Institute of Science and Technology , Seoul 02792 , South Korea.
Nano Lett ; 19(6): 3692-3698, 2019 06 12.
Article em En | MEDLINE | ID: mdl-31084032
ABSTRACT
Because of its effectiveness in blocking electrons, the solid electrolyte interface (SEI) suppresses decomposition reactions of the electrolyte and contributes to the stability and reversibility of batteries. Despite the critical role of SEI in determining the properties of batteries, the electrical properties of SEI layers have never been measured directly. In this paper, we present the first experimental results of the electrical resistivity of a LiF-rich SEI layer measured using a direct-contact microelectrical device mounted in an electron microscope. Measurements show that the SEI layer exhibits high electrical resistivity (2.3 × 105 Ω·m), which is comparable with those of typical insulating materials. Furthermore, a combined technique of advanced analyses and first-principles calculations show that the SEI layer is mainly composed of amorphous LiF and a minute nanocrystalline Li2CO3 compound. The electronic origin responsible for the high resistivity of the SEI layer is elucidated by calculating the band structures of various Li xF compounds and interpreting their effects on the resistivity. This study explains why SEI can prevent the degradation of electrode materials and consumption of Li ions in the electrolyte and thus can be viewed as a stepping stone for developing highly stable and reversible batteries.