Development of the PVA/CS nanofibers containing silk protein sericin as a wound dressing: In vitro and in vivo assessment.
Bakhsheshi-Rad, Hamid Reza; Ismail, Ahmad Fauzi; Aziz, Madzlan; Akbari, Mohsen; Hadisi, Zhina; Omidi, Mahdi; Chen, Xiongbiao.
Afiliação
  • Bakhsheshi-Rad HR; Advanced Materials Research Center, Department of Materials Engineering, Najafabad Branch, Islamic Azad University, Najafabad, Iran; Advanced Membrane Technology Research Center (AMTEC), Universiti Teknologi Malaysia, 81310, Skudai, Johor Bahru, Johor, Malaysia. Electronic address: rezabakhsheshi@pm
  • Ismail AF; Advanced Membrane Technology Research Center (AMTEC), Universiti Teknologi Malaysia, 81310, Skudai, Johor Bahru, Johor, Malaysia.
  • Aziz M; Advanced Membrane Technology Research Center (AMTEC), Universiti Teknologi Malaysia, 81310, Skudai, Johor Bahru, Johor, Malaysia.
  • Akbari M; Laboratory for Innovations in MicroEngineering (LiME), Department of Mechanical Engineering, University of Victoria, Victoria, BC V8P 5C2, Canada.
  • Hadisi Z; Laboratory for Innovations in MicroEngineering (LiME), Department of Mechanical Engineering, University of Victoria, Victoria, BC V8P 5C2, Canada.
  • Omidi M; Advanced Materials Research Center, Department of Materials Engineering, Najafabad Branch, Islamic Azad University, Najafabad, Iran.
  • Chen X; Department of Mechanical Engineering, College of Engineering, University of Saskatchewan, Saskatoon, SK, Canada.
Int J Biol Macromol ; 149: 513-521, 2020 Apr 15.
Article em En | MEDLINE | ID: mdl-31954780
Skin and soft tissue infections are major concerns with respect to wound repair. Recently, anti-bacterial wound dressings have been emerging as promising candidates to reduce infection, thus accelerating the wound healing process. This paper presents our work to develop and characterize poly(vinyl alcohol) (PVA)/chitosan (CS)/silk sericin (SS)/tetracycline (TCN) porous nanofibers, with diameters varying from 305 to 425 nm, both in vitro and in vivo for potential applications as wound dressings. The fabricated nanofibers possess a considerable capacity to take up water through swelling (~325-650%). Sericin addition leads to increased hydrophilicity and elongation at break while decreasing fiber diameter and mechanical strength. Moreover, fibroblasts (L929) cultured on the nanofibers with low sericin content (PVA/CS/1-2SS) displayed greater proliferation compared to those on nanofibers without sericin (PVA/CS). Nanofibers loaded with high sericin and tetracycline content significantly inhibited the growth of Escherichia coli and Staphylococcus aureus. In vivo examination revealed that PVA/CS/2SS-TCN nanofibers enhance wound healing, re-epithelialization, and collagen deposition compared to traditional gauze and nanofibers without sericin. The results of this study demonstrate that the PVA/CS/2SS-TCN nanofiber creates a promising alternative to traditional wound dressing materials.
Assuntos
Palavras-chave

Texto completo: 1 Base de dados: MEDLINE Assunto principal: Cicatrização / Seda / Sericinas / Antibacterianos Limite: Animals / Humans Idioma: En Ano de publicação: 2020 Tipo de documento: Article

Texto completo: 1 Base de dados: MEDLINE Assunto principal: Cicatrização / Seda / Sericinas / Antibacterianos Limite: Animals / Humans Idioma: En Ano de publicação: 2020 Tipo de documento: Article