Your browser doesn't support javascript.
loading
Influence of the degree of conversion and Bis-GMA residues of bulk fill resins on tissue toxicity in an subcutaneous model in rats.
Barreto Girão, Liliana; Ohana de Lima Martins, Joyce; Lemos, José Vitor Mota; Pinto, Marcílio Rodrigues; Rolim, Juliana Paiva Marques Lima; Alves E Silva, Francisco Cláudio Fernandes; Saboia, Vicente de Paulo Aragão; Bitu Sousa, Fabrício; de Barros Silva, Paulo Goberlânio.
Afiliação
  • Barreto Girão L; Department of Dentistry, Unichristus, Fortaleza, Ceará, Brazil.
  • Ohana de Lima Martins J; Department of Dentistry, Unichristus, Fortaleza, Ceará, Brazil.
  • Lemos JVM; Department of Clinic Dentistry, Federal University of Ceará, Fortaleza, Ceará, Brazil.
  • Pinto MR; Department of Dentistry, Unichristus, Fortaleza, Ceará, Brazil.
  • Rolim JPML; Department of Dentistry, Unichristus, Fortaleza, Ceará, Brazil.
  • Alves E Silva FCF; Department of Dentistry, Unichristus, Fortaleza, Ceará, Brazil.
  • Saboia VPA; Department of Dentistry, Unichristus, Fortaleza, Ceará, Brazil.
  • Bitu Sousa F; Department of Restorative Dentistry, Federal University of Ceará, Fortaleza, Ceará, Brazil.
  • de Barros Silva PG; Department of Dentistry, Unichristus, Fortaleza, Ceará, Brazil.
J Appl Biomater Funct Mater ; 18: 2280800020947330, 2020.
Article em En | MEDLINE | ID: mdl-33151768
ABSTRACT

AIM:

To analyse the influence of the degree of conversion (DC) and light curing residues of different bulk fills (BFs) composites on the inflammatory profile in the subcutaneous tissue of rats. MATERIALS AND

METHODS:

Resin disks of BF-resins and their active conventional resins (CR; 3M®, Ivoclar®, and Kerr®) were light-cured at 2 mm (BF-superficial) and 4 mm (BF-deep) thicknesses and analyzed by infrared spectroscopy (FTIR; n = 3/group; DC and light curing residues). Then, the disks were implanted in four quadrants in the subcutaneous tissue of Wistar rats (sham, CR, BF-superficial and RF-deep), and after 7, 14, and 28 days, the animals (n = 6/day) were euthanized for histological analysis of the intensity of the inflammatory process (scores 0-3). Kruskal-Wallis/Dunn and ANOVA/Bonferroni tests were used (p < 0.05, Graph Pad Prism 5.0).

RESULTS:

The DC of CR 3M® did not differ significantly compared to BF-superficial and BF-deep resins (p = 0.235). The Ivoclar® and Kerr® resins showed a higher DC with CR and BF-superficial compared to the BF-deep (p = 0.005 and p = 0.011, rctively). Kerr® resins showed a higher Bis-GMA/UDMA ratio, especially in BF-deep resin (p < 0.05). 3M® and Ivoclar resins did not show high inflammation scores, but for Kerr® BF resins (superficial and deep), the inflammatory process was significantly higher than that in the CR and sham quadrants (p = 0.031).

CONCLUSION:

The tissue inflammatory response after resin inoculation depends on the DC and light curing residues of Bis-GMA.
Assuntos
Palavras-chave

Texto completo: 1 Base de dados: MEDLINE Assunto principal: Materiais Biocompatíveis / Bis-Fenol A-Glicidil Metacrilato / Resinas Compostas / Materiais Dentários / Inflamação Tipo de estudo: Prognostic_studies Limite: Animals Idioma: En Ano de publicação: 2020 Tipo de documento: Article

Texto completo: 1 Base de dados: MEDLINE Assunto principal: Materiais Biocompatíveis / Bis-Fenol A-Glicidil Metacrilato / Resinas Compostas / Materiais Dentários / Inflamação Tipo de estudo: Prognostic_studies Limite: Animals Idioma: En Ano de publicação: 2020 Tipo de documento: Article