Your browser doesn't support javascript.
loading
Palladium/Ferrierite versus Palladium/SSZ-13 Passive NOx Adsorbers: Adsorbate-Controlled Location of Atomically Dispersed Palladium(II) in Ferrierite Determines High Activity and Stability.
Khivantsev, Konstantin; Wei, Xinyi; Kovarik, Libor; Jaegers, Nicholas R; Walter, Eric D; Tran, Pascaline; Wang, Yong; Szanyi, János.
Afiliação
  • Khivantsev K; Institute for Integrated Catalysis, Pacific Northwest National Laboratory, Richland, WA, 99352, USA.
  • Wei X; Environmental Catalysis Research Division, BASF, Iselin, NJ, 08830, USA.
  • Kovarik L; Institute for Integrated Catalysis, Pacific Northwest National Laboratory, Richland, WA, 99352, USA.
  • Jaegers NR; Institute for Integrated Catalysis, Pacific Northwest National Laboratory, Richland, WA, 99352, USA.
  • Walter ED; Institute for Integrated Catalysis, Pacific Northwest National Laboratory, Richland, WA, 99352, USA.
  • Tran P; Environmental Catalysis Research Division, BASF, Iselin, NJ, 08830, USA.
  • Wang Y; Institute for Integrated Catalysis, Pacific Northwest National Laboratory, Richland, WA, 99352, USA.
  • Szanyi J; Voiland School of Chemical Engineering and Bioengineering, Washington State University, Pullman, WA, 99164, USA.
Angew Chem Int Ed Engl ; 61(3): e202107554, 2022 Jan 17.
Article em En | MEDLINE | ID: mdl-34617372
ABSTRACT
Pd-loaded FER and SSZ-13 zeolites as low-temperature passive NOx adsorbers (PNA) are compared under practical conditions. Vehicle cold start exposes the material to CO under a range of concentrations, necessitating a systematic exploration of the effect of CO on the performance of isolated Pd ions in PNA. The NO release temperature of both adsorbers decreases gradually with an increase in CO concentration from a few hundred to a few thousand ppm. This beneficial effect results from local nano-"hot spot" formation during CO oxidation. Dissimilar to Pd/SSZ-13, increasing the CO concentration above ≈1000 ppm improves the NOx storage significantly for Pd/FER, which was attributed to the presence of Pd ions in FER sites that are shielded from NOx. CO mobilizes this Pd atom to the NOx accessible position where it becomes active for PNA. This behavior explains the very high resistance of Pd/FER to hydrothermal aging Pd/FER materials survive hydrothermal aging at 800 °C in 10 % H2 O vapor for 16 hours with no deterioration in NOx uptake/release behavior. Thus, by allocating Pd ions to the specific microporous pockets in FER, we have produced (hydro)thermally stable and active PNA materials.