Real-time monitoring of aqueous Hg2+ reduction dynamics by magnetite/iron metal composite powders synthesized hydrothermally.
Brunet, Fabrice; Tisserand, Delphine; Lanson, Martine; Malvoisin, Benjamin; Bertrand, Mathieu; Bonnaud, Céline.
Afiliação
  • Brunet F; ISTERRE, Univ. Grenoble Alpes, Univ. Savoie Mont Blanc, CNRS, IRD, Univ. Gustave Eiffel, Grenoble 38000, France E-mail: fabrice.brunet@univ-grenoble-alpes.fr.
  • Tisserand D; ISTERRE, Univ. Grenoble Alpes, Univ. Savoie Mont Blanc, CNRS, IRD, Univ. Gustave Eiffel, Grenoble 38000, France E-mail: fabrice.brunet@univ-grenoble-alpes.fr.
  • Lanson M; ISTERRE, Univ. Grenoble Alpes, Univ. Savoie Mont Blanc, CNRS, IRD, Univ. Gustave Eiffel, Grenoble 38000, France E-mail: fabrice.brunet@univ-grenoble-alpes.fr.
  • Malvoisin B; ISTERRE, Univ. Grenoble Alpes, Univ. Savoie Mont Blanc, CNRS, IRD, Univ. Gustave Eiffel, Grenoble 38000, France E-mail: fabrice.brunet@univ-grenoble-alpes.fr.
  • Bertrand M; HYMAG'IN, Grenoble 38000, France.
  • Bonnaud C; HYMAG'IN, Grenoble 38000, France.
Water Sci Technol ; 86(3): 596-609, 2022 Aug.
Article em En | MEDLINE | ID: mdl-35960839
ABSTRACT
An iron-based powder material composed of zerovalent iron (8 wt.%) and magnetite (92 wt.%), has been synthesized hydrothermally at 200 °C from zero-valent iron. Its effect on the reduction of aqueous Hg2+ into gaseous Hg0 has been investigated at ambient conditions for pH comprised between 4 and 8.5. The production of Hg0 was monitored with an online mercury vapor analyzer at the picogram level for concentrations of iron-based composite of a few tenths of mg L-1. Starting from a solution having an Hg2+ concentration of 25 ng L-1 at pH = 4, a succession of two Hg0 production events was recorded. The first event is related to the Hg2+ reduction by ZVI which fully dissolved within the first hours. Upon ZVI consumption, pH drifted towards the pH window where magnetite can efficiently reduce Hg2+ at the hour timescale, resulting in a second Hg0 production peak. The combined use of ZVI and magnetite to remove aqueous Hg2+ by formation of Hg0 (volatile) under mild acidic pH allows (1) to maximize the Hg2+ reduction rate and (2) to take benefit of the longer lifetime of magnetite compared to ZVI.