Your browser doesn't support javascript.
loading
Redox-triggered debonding of mussel-inspired pressure sensitive adhesives: Improving efficiency through functional design.
Neubert, Tilmann J; Walter, Keven; Schröter, Carolin; Guglielmotti, Victoria; Hinrichs, Karsten; Reinicke, Stefan; Taden, Andreas; Balasubramanian, Kannan; Börner, Hans G.
Afiliação
  • Neubert TJ; Humboldt-Universität zu Berlin, Department of Chemistry, GERMANY.
  • Walter K; Humboldt-Universität zu Berlin, Department of Chemistry, GERMANY.
  • Schröter C; Humboldt-Universität zu Berlin, Department of Chemistry, GERMANY.
  • Guglielmotti V; Universidad Nacional de General San Martin, Instituto de Nanosistemas, GERMANY.
  • Hinrichs K; Leibniz-Institut fur Analytische Wissenschaften - ISAS eV Department Berlin, ISAS, GERMANY.
  • Reinicke S; Fraunhofer Institute for Applied Polymer Research IAP, Polymer Chemistry, GERMANY.
  • Taden A; Henkel AG & Co. KGaA, Adhesive Research, GERMANY.
  • Balasubramanian K; Humboldt-Universität zu Berlin, Analytical Sciences Adlershof (SALSA), GERMANY.
  • Börner HG; Humboldt-Universitat zu Berlin, Department of Chemistry, Brook-Taylor-Str. 2, 12489, Berlin, GERMANY.
Angew Chem Int Ed Engl ; : e202408441, 2024 Jul 27.
Article em En | MEDLINE | ID: mdl-39072978
ABSTRACT
Debondable pressure-sensitive adhesives (PSAs) promise access to recyclability in microelectronics in the transition toward a circular economy. Two PSAs were synthesized from a tetravalent thiol star-polyester forming thiol-catechol-connectivities (TCC) with either biorelated DiDopa-bisquinone (BY*Q) or fossil-based bisquinone A (BQA). The PSAs enable debonding by oxidation of TCC-catechols to quinones. The extent of debonding efficiency depends on the interaction modes, which are determined by the chemical structure differences of both TCC-motifs. BY*Q-TCC-PSA debonds with exceptional loss of 99% of its approx. 2 MPa shear strength. For BQA-TCC-PSA, a debonding efficiency of only approx. 60% was found, irrespective of its initial shear strength, which could be tuned up to approx. 7 MPa. The efficiency of debonding for BY*Q-TCC-PSA after TCC-oxidation is linked to the loss of synergistic interactions without strongly affecting the bulk glue properties, outperforming the purely catechol-based BQA-analogue.
Palavras-chave

Texto completo: 1 Base de dados: MEDLINE Idioma: En Ano de publicação: 2024 Tipo de documento: Article

Texto completo: 1 Base de dados: MEDLINE Idioma: En Ano de publicação: 2024 Tipo de documento: Article