Detalhe da pesquisa
1.
Disentangling Phase and Morphological Evolution During the Formation of the Lithium Superionic Conductor Li10 GeP2 S12.
Small
; 19(28): e2300850, 2023 Jul.
Artigo
em Inglês
| MEDLINE | ID: mdl-36974581
2.
Capacity Degradation of Zero-Excess All-Solid-State Li Metal Batteries Using a Poly(ethylene oxide) Based Solid Electrolyte.
ACS Appl Mater Interfaces
; 2024 Jun 11.
Artigo
em Inglês
| MEDLINE | ID: mdl-38863333
3.
Li-Ion Conductivity of Single-Step Synthesized Glassy-Ceramic Li10GeP2S12 and Post-heated Highly Crystalline Li10GeP2S12.
ACS Appl Mater Interfaces
; 15(29): 34973-34982, 2023 Jul 26.
Artigo
em Inglês
| MEDLINE | ID: mdl-37442800