RESUMO
Wire-feed additive manufacturing (WFAM) produces superalloys with complex thermal cycles and unique microstructures, often requiring optimized heat treatments. To address this challenge, we present a hybrid approach that combines high-throughput experiments, precipitation simulation, and machine learning to design effective aging conditions for the WFAM Haynes 282 superalloy. Our results demonstrate that the γ' radius is the critical microstructural feature for strengthening Haynes 282 during post-heat treatment compared with the matrix composition and γ' volume fraction. New aging conditions at 770°C for 50 hours and 730°C for 200 hours were discovered based on the machine learning model and were applied to enhance yield strength, bringing it on par with the wrought counterpart. This approach has significant implications for future AM alloy production, enabling more efficient and effective heat treatment design to achieve desired properties.
Our research tackles suboptimal properties in additively manufactured alloys with conventional heat treatment, using high-throughput experiments, CALPHAD (CALculation of PHAse Diagrams), and interpretable machine learning to effectively optimize heat treatments for WFAM (Wire-Feed Additive Manufacturing) Haynes 282 superalloy.
RESUMO
The segregation of reactive elements (REs) along thermally grown oxide (TGO) grain boundaries has been associated to slower oxide growth kinetics and improved creep properties. However, the incorporation and diffusion of these elements into the TGO during oxidation of Ni alloys remains an open question. In this work, electron backscatter diffraction in transmission mode (t-EBSD) was used to investigate the microstructure of TGO within the thermal barrier coating on a Ni-based superalloy, and atom probe tomography (APT) was used to quantify the segregation behavior of REs to α-Al2O3 grain boundaries. Integrating the two techniques enables a higher level of site-specific analysis compared to the routine focused ion beam lift-out sample preparation method without t-EBSD. Needle-shaped APT specimens readily meet the thickness criterion for electron diffraction analysis. Transmission EBSD provides an immediate feedback on grain orientation and grain boundary location within the APT specimens to help target grain boundaries in the TGO. Segregation behavior of REs is discussed in terms of the grain boundary character and relative location in TGO.
RESUMO
Plasma focused ion beam microscopy (PFIB) is a recent nanofabrication technique that is suitable for site-specific atom probe sample preparation. Higher milling rates and fewer artifacts make it superior to Ga+ FIBs for the preparation of samples where large volumes of material must be removed, for example, when trying to avoid lift-out techniques. Transmission Kikuchi diffraction (TKD) is a method that has facilitated phase identification and crystallographic measurements in such electron transparent samples. We propose a procedure for preparing atom probe tomography (APT) tips from mechanically prepared ribbons by using PFIB. This is highly suitable for the preparation of atom probe tips of interfaces such as interphase boundaries from challenging materials where lift-out tips easily fracture. Our method, in combination with TKD, allows the positioning of regions of interest such as interfaces close to the apex of the tip. We showcase the efficacy of the proposed method in a case study on Alloy 718, where the interface between γ-matrix and δ-phase has not been yet extensively explored through APT due to preparation challenges. Results show depletion of γâ³-precipitates near the γ/δ interface. A quantitative evaluation of the composition of phases in the bulk versus near the interface is achieved.
RESUMO
Polycrystalline Ni-based superalloys for aerospace and power generation applications are often precipitation hardened to achieve strengthening at elevated temperatures. Here, atom probe microscopy has become an essential tool to study the complex morphology of nanoscale precipitates. This study focuses on Alloy 718, which is hardened by semi-coherent, ordered γ' (Ni3(Al, Ti)) and γⳠ(Ni3(Nb)) particles. According to previous research, these particles often occur as duplets or triplets with a stacking sequence dependent on prior processing. This creates various interfaces with a strong impact on the mechanical properties, highlighting the importance of quantitative studies which are challenging with electron microscopy. We present atom probe data reconstruction and analysis approaches particularly suited for precipitation hardened superalloys. While voltage atom probe allows for an accurate reconstruction, the acquired data volume is often limited. Laser-assisted atom probe provides statistically significant data, but the loss of crystallographic information requires correlation with voltage-mode datasets. We further describe an advanced iso-surface method where initially arbitrarily chosen concentration thresholds of Al + Ti for γ' and Nb for γⳠparticles are optimized. Recognizing the importance of the precipitate stacking order, the different types of precipitate interfaces are quantified, and these methods may be applicable to other engineering alloys.
RESUMO
The synergistic effects of boron (B) and rare earth (RE) elements on the microstructure and stress rupture properties were investigated in a Ni-based superalloy. The stress rupture lifetime at 650 °C/873 MPa significantly increased with the addition of B as a single element. Furthermore, the stress rupture lifetime reached its peak (303 h), with a certain amount of B and RE added together in test alloys. Although the grain size and morphology of the γ' phase varied a little with the change in B and RE addition, they were not considered to be the main reasons for stress rupture performance. The enhancement in stress rupture lifetime was mostly attributed to the segregation of the B and RE elements, which increased the binding force of the grain boundary and improved its strength and plasticity. In addition, the enrichment of B and RE inhabited the precipitation of carbides along grain boundaries. Furthermore, nano-scale RE precipitates containing sulfur (S) and phosphorus (P) were observed to be distributed along the grain boundaries. The purification of grain boundaries by B and RE elements was favorable to further improve the stress rupture properties.
RESUMO
The effect of the active element yttrium and its content on the oxidation behavior of GH4169 Ni-based superalloy at extreme temperature was studied by isothermal oxidation experiments. The results show that the oxide scale of GH4169 alloy presents a multi-layer structure, in which the continuous and dense Cr2O3 oxide layer is located in the subouter layer (II layer) and the continuous Nb-rich layer is in the subinner layer (III layer). These layers can inhibit the diffusion of oxygen and alloying elements, preventing the further oxidation of the alloy. The appropriate addition of yttrium can promote the selective oxidation of Cr element, reduce the thickness of the oxide scale and the oxidation rate of the alloy, inhibit the formation of voids at the interface of the oxide scale/alloy matrix, improve the resistance of the alloy to spalling as well as the adhesion of the oxide scale, and improve the high-temperature oxidation resistance of the alloy. Of those tested, the alloy containing 0.04 wt.%Y has the lowest oxidation weight gain, the slowest oxidation rate, and less oxide scale spalling. Based on this, the effect of yttrium on the high-temperature oxidation behavior of GH4169 Ni-based superalloy and its mechanism were revealed.
RESUMO
The solution heat treatment (SHT) of the third generation of single crystal (SC) Ni-based superalloys required up to 45 h and was expensive. In this study, SHT based on liquid metal cooling (LMC) was optimized to greatly reduce processing time. The experimental and simulation results showed that residual segregation was evidently reduced, e.g., from 2.12 to 1.22 for the most heavily segregated Re. This led to a 16.7% increase in creep life, more uniform microstructures, and a decrease in solidification and homogenization porosity by a factor of 3.4. Structural refinement, approximately 0.32 times, served as the underlying mechanism for this optimization, which reduced diffusion distance and increased homogenization efficiency during SHT.
RESUMO
In this study, nine as-cast Ni-Al-Cr-Os alloys were prepared, and their constituent phases and microstructure were examined using X-ray diffraction and electron probe microanalysis techniques. The solidification paths of all the alloys in a Ni-rich corner were revealed based on a detailed analysis of the as-cast microstructure. The liquidus cube of the quaternary Ni-Al-Cr-Os system in a Ni-rich corner was established accordingly. A eutectic-type invariant reaction on the liquidus surface was explicitly identified, and its reaction can be expressed as L â α + ß + γ. No quaternary invariant reaction was found in the alloys following the addition of Os. The Ni-Al-Cr-Os alloy points were then vertically mapped onto the Ni-Al-Cr liquid phase projection to better observe the effect of Os addition on the solidification path of the Ni-Al-Cr system. It was found that the addition of a small amount of Os has no significant effect on the solidification path of the Ni-Al-Cr system. Furthermore, the microhardness of each alloy, which was determined to be in the range of 207 HV to 565 HV, was found to be closely related to the phase constitution and phase fraction of the alloy.
RESUMO
The present study investigates the creep behavior and deformation mechanism of a third-generation single-crystal Ni-based superalloy at 1170 °C under a range of stress levels. Scanning electron microscopes (SEM) and transmission electron microscopes (TEM) were employed to observe the formation of a rafted γ' phase, which exhibits a topologically close-packed (TCP) structure. The orientation relationship and elemental composition of the TCP phase and matrix were analyzed to discern their impact on the creep properties of the alloy. The primary deformation mechanism of the examined alloy was identified as dislocation slipping within the γ matrix, accompanied by the climbing of dislocations over the rafted γ' phase during the initial stage of creep. In the later stages of creep, super-dislocations with Burgers vectors of a<010> and a/2<110> were observed to shear into the γ' phase, originating from interfacial dislocation networks. Up to the fracture, the sequential activation of dislocation shearing in the primary and secondary slipping systems of the γ' phase occurs. As a consequence of this alternating dislocation shearing, a twist deformation of the rafted γ' phase ensued, ultimately contributing to the fracture mechanism observed in the alloy during creep.
RESUMO
The Si atom diffusion behavior in Ni-based superalloys was evaluated based on first-principles calculations. Also, the site occupation of Si atoms as the melting point depressant elements in Cr, Mo, and W atom doped γ-Ni and γ'-Ni3Fe supercells was discussed and Si atom diffusion behaviors between both adjacent octahedral interstices were analyzed. Calculation results indicated that formation enthalpy (∆Hf) was decreased, stability was improved by doping alloying elements Cr, Mo, and W in γ-Ni and γ'-Ni3Fe supercells, Si atoms were more inclined to occupy octahedral interstices and the diffusion energy barrier was increased by increasing the radius of the doped alloy element. Especially, two diffusion paths were available for Si atoms in the γ'-Ni3Fe and Si diffusion energy barrier around the shared Fe atoms between adjacent octahedral interstices and was significantly lower than that around the shared Ni atoms. The increase of interaction strength between the doped M atom/octahedron constituent atom and Si atom increased Si atom diffusion and decreased the diffusion energy barrier. The Si atom diffusion behavior provides a theoretical basis for the phase structure evolution in wide-gap brazed joints.
RESUMO
Wire arc additively manufactured (WAAM) Ni-based materials have good properties but are costly and hard to cut, leading to difficulties in machining after welding and wasting the materials. To overcome these shortcomings, this work proposes a method of surfacing Fe-based alloy layers on WAAM Ni-based material. The effect of this method on the microstructure and wear properties of WAAM Ni-based materials is discussed. In this work, a Fe-based alloy (JX103) was welded as the last layers of the WAAM Ni-based superalloy (JX201) material. The hardness, microstructure, and wear behavior of the material with different residual Fe-based materials were tested and analyzed. Our results indicate that the surface hardness was smoothly increased from HV350 to HV400 by overlaying Fe-based alloy layers. Microstructure analysis shows that γ-Fe gradually disappears, and the carbide form changes from WAAM Ni-based superalloys to Fe-based alloys. In the fusion boundary, the occurrence of cellular dendritic growth, a type -⠡ boundary, and low dilution indicate good crack resistance and good connection performance between these two materials. The wear test showed that the wear resistance of JX201 was decreased by changing the last layer to JX103. However, as the residual thickness of JX103 decreased, the influence gradually reduced. Meanwhile, the wear mechanism changed from severe abrasive and adhesive wear to light abrasive wear. When the thickness is less than 0.5 mm, the wear weight per minute is at the same level as the sample without JX103.
RESUMO
A Ni25-10% SiC-X% graphene (mass fraction X = 0, 0.5, 1.0, 1.5) composite cladding layer was prepared on a 6063 aluminum alloy substrate using laser cladding in order to enhance the comprehensive performance of the aircraft refueling interface. The effect of the graphene content on the organization and properties of nickel-based silicon carbide composite cladding layers was investigated by laser melting. The macroscopic morphology, microstructure, hardness, elemental changes, corrosion and wear resistance of the cladding layer were studied by optical microscopy, scanning electron microscopy, a hardness tester, an X-ray diffractometer, an electrochemical workstation and an M-2000 frictional wear tester. The results indicated that the nickel-based clad layer without graphene incorporation had the worst forming, with a large number of pores and cracks in the cladding layer. Because graphene agglomerated easily, cracks were regenerated when the content of graphene was higher than 0.5%. The material phases of the cladding layer without graphene incorporation were mainly: Al3Ni2, Fe3Si and SiC. Due to the addition of graphene, the clad layer of specimen 2 was refined and a large number of hard phases, such as CrC and Cr23C6, were generated, which led to the increase in the hardness of the clad layer. When the content of graphene was further increased, the number of hard phases such as CrC and Cr23C6 produced in the cladding was relatively reduced due to the agglomeration of graphene, and the hardness of the cladding was reduced. As the impermeability of graphene reduces the diffusion of corrosive media to the substrate, the generation of hard-phase Al3Ni2 in the cladding layer makes the corrosion resistance of the cladding layer increase with the increase in graphene mass fraction. The result is that, when the content of graphene was 0.5%, the overall performance of the clad layer was the best, where its average hardness was increased by 40%, the average coefficient of friction was reduced by 12.7% and the wear rate was reduced by 60%.
RESUMO
The DD407 single crystal Ni-based superalloy with a face-centered cubic structure exhibits strong anisotropic characteristics. In order to reveal the material chip formation mechanism and the impact effect of crystal orientations on the materials' milling machinability, a combination of experimental observations and theoretical analysis were applied in this study. Considering the resolved shear stress and slip system theories, a fundamental theoretical explanation of the milling force and surface quality along different crystal directions on the (001) crystal plane of the DD407 single crystal Ni-based superalloy was proposed based on a previously constructed anisotropic milling model. Our work in this research verifies that [110] crystal direction on the (001) crystal plane of the DD407 single crystal Ni-based superalloy is the most optimal feeding direction during milling, taking into account surface roughness and morphology, slot bottom plastic deformation, work hardening, and chip edge burr feature.
RESUMO
The single-crystal Ni-based superalloys, which have excellent mechanical properties at high temperatures, are commonly used for turbine blades in a variety of aero engines and industrial gas turbines. Focusing on the phase interface of a second-generation single-crystal Ni-based superalloy, in-situ TEM observation was conducted at room temperature and high temperatures. Intensity ratio analysis was conducted for the measurement of two-phase interface width. The improved geometric phase analysis method, where the adaptive mask selection method is introduced, was used for the measurement of the strain field near the phase interface. The strained irregular transition region is consistent with the calculated interface width using intensity ratio analysis. An intensity ratio analysis and strain measurement near the interface can corroborate and complement each other, contributing to the interface structure evaluation. Using TEM in-situ heating and Fourier transform, the change of dislocation density in the γ phase near the two-phase interface of the single-crystal Ni-based superalloy was analyzed. The dislocation density decreases first with the increase in temperature, consistent with the characteristics of metal quenching, and increases sharply at 450 °C. The correlation between the variation of dislocation density at high temperatures and the intermediate temperature brittleness was also investigated.
RESUMO
The Portevin-Le Châtelier (PLC) effect in a powder metallurgy (PM) Co-Ni-based superalloy was systematically investigated via the tensile tests at temperatures ranging from 200 to 600 °C and strain rates at 1.0 × 10-4 to 1.0 × 10-2. Both normal and inverse PLC effects were observed in the PLC regime, and the former appeared in the A and B types at a low temperature, whilst the latter appeared in the C type at an elevated temperature. Both positive and negative strain rate sensitivities (SRS) were shown in PLC regime, and SRS should be derived from same types of serrations. Based on the calculated activation energy, the substitutional atom Mo is considered to take primary responsibility for the PLC effect in present alloy.
RESUMO
The grain growth behavior in a typical Ni-based superalloy was investigated using isothermal heat treatment experiments over a holding temperature range of 1353-1473 K. The experimental results showed that the grain structure continuously coarsened as the holding time and holding temperature increased during heat treatment. A classical parabolic grain growth model was used to explore the mechanism of grain growth under experimental conditions. The grain growth exponent was found to be slightly above 2. This indicates that the current grain growth in the studied superalloy is mainly governed by grain boundary migration with a minor pinning effect from the precipitates. Then, the grain growth in the studied superalloy during isothermal heat treatment was modelled by a cellular automaton (CA) with deterministic state switch rules. The microscale kinetics of grain growth is described by the correlation between the moving velocity and curvature of the grain boundary. The local grain boundary curvature is well evaluated by a template disk method. The grain boundary mobility was found to increase with increasing temperature. The relationship between the grain boundary mobility and temperature has been established. The developed CA model is capable of capturing the dependence of the grain size on the holding time under different holding temperatures.
RESUMO
Using suitable scanning strategies, even single crystals can emerge from powder during additive manufacturing. In this paper, a full microstructure map for additive manufacturing of technical single crystals is presented using the conventional single crystal Ni-based superalloy CMSX-4. The correlation between process parameters, melt pool size and shape, as well as single crystal fraction, is investigated through a high number of experiments supported by numerical simulations. Based on these results, a strategy for the fabrication of high fraction single crystals in powder bed fusion additive manufacturing is deduced.
RESUMO
Higher fatigue and creep resistance at high temperatures are the essential properties for materials such as those used in gas turbines for power generation and aircraft turbines. Therefore, the nickel-based superalloy CMSX-4 was developed through single-crystal casting to satisfy these requirements. In this study, the CMSX-4 creep test results reported by previous researchers were used to mathematically derive an equation to estimate the amount of creep damage occurring under variable load conditions. In addition, low-cycle fatigue tests were performed, and the effect of creep damage occurring during fatigue on material failure was described.
RESUMO
The present work demonstrates a technique for the hot forging of metal surfaces in water at 1000 °C or higher, termed energy-intensive multifunctional cavitation (EI-MFC). In this process, the energy of cavitation bubbles is maximized, following which these bubbles collide with the metal surface. This technique will be employed to improve the surface structure of CM186LC/DS, a Ni-based columnar crystalline superalloy used to manufacture the rotor blades of jet engines and gas turbines that are exposed to high-temperature oxidizing environments, with the aim of improving creep strength. EI-MFC processing induces compressive residual stress in the metal that prevents the occurrence of surface cracks and also increases surface hardness, improves corrosion resistance, and increases the coefficient of friction. The latter effect can enhance the adhesion of thermal barrier coatings applied to Ni-based superalloys by thermal spraying. The technology demonstrated herein can be applied to present-day jet engine and gas turbine components and also to the production of hydrogen combustion turbines operating at 1700 °C with higher combustion efficiency than the current 1500 °C class gas turbines. In addition, the high processing energy obtained using the EI-MFC technique has the potential to flatten rough surfaces resulting from the stacking pitches of various metals manufactured using three-dimensional printers, and so improve surface strength.
RESUMO
Ni-based superalloy with ceramic thermal barrier coatings (TBCs) is a composite material, which can be used in special environments with high temperature and high pressure such as aeroengine blade. In order to improve the cooling effect of the aeroengine, it is necessary to perform multi-size and large-area holes processing on the surface of blades. As a non-contact processing method with fast processing speed, good processing quality and almost no deformation, laser processing has been one of the important processing methods for film cooling hole processing of aeroengine blades. Percussion drilling is presented using picosecond ultrashort pulse laser in order to explore processing of deep holes in Ni-based superalloy, ceramic TBCs, and ceramic TBCs/substrate multilayer material. The effects of pulses, threshold and wavelength on hole diameter have been discussed, and the experiment on the deep hole ablation with 1064 nm wavelength has been performed. By analyzing the hole size and morphological characteristics of multiple processing parameters, the variation of hole cylindricity is obtained. A high-quality hole, without spatters around the periphery of hole entrance and without recast layer on the side-wall surface, in Ni-based superalloy coated with ceramic TBCs has been drilled. This research has potential applications to blade film cooling holes.