In vitro degradation of resin-dentin bonds with one-bottle self-etching adhesives.
Eur J Oral Sci
; 117(5): 611-7, 2009 Oct.
Article
em En
| MEDLINE
| ID: mdl-19758260
ABSTRACT
The purpose of this study was to evaluate the durability of one-bottle self-etching adhesive during long-term water-storage testing. Resin-dentin bonded specimens were prepared using four commercially available one-bottle self-etching adhesives. The specimens were sectioned perpendicular to the adhesive interface to produce beam-shaped specimens that were stored in water for 24 h (control group) and 100, 200, and 300 d (experimental groups). After each storage period, the beams were subjected to a microtensile bond test. After the bond test, fractured surfaces were examined using a scanning electron microscope. In addition, interfacial observations of the silver tracer were performed using the secondary and back-scatter modes of the scanning electron microscope. The bond strength of all tested adhesives decreased significantly after 100 or more days in water. The interfacial observations showed an oxygen-inhibition zone as electron lucent in the adhesive-composite border in control specimens, displaying silver impregnation with breakage after aging. The deterioration of the oxygen-inhibition zone in the adhesive-resin composite junction resulted in a decrease in bond strength after 100 d in water for one-bottle self-etching adhesives.
Texto completo:
1
Coleções:
01-internacional
Base de dados:
MEDLINE
Assunto principal:
Colagem Dentária
/
Adesivos Dentinários
/
Resinas Compostas
/
Materiais Dentários
/
Dentina
Limite:
Humans
Idioma:
En
Ano de publicação:
2009
Tipo de documento:
Article