Your browser doesn't support javascript.
loading
Radiative dynamics and delayed emission in pure and doped InP/ZnSe/ZnS quantum dots.
Cavanaugh, Paul; Sun, Haochen; Jen-La Plante, Ilan; Bautista, Maria J; Ippen, Christian; Ma, Ruiqing; Kelley, Anne Myers; Kelley, David F.
Afiliação
  • Cavanaugh P; Chemistry and Biochemistry, University of California Merced, 5200 North Lake Road, Merced, California 95343, USA.
  • Sun H; Chemistry and Biochemistry, University of California Merced, 5200 North Lake Road, Merced, California 95343, USA.
  • Jen-La Plante I; Nanosys, Inc., 233 S. Hillview Dr., Milpitas, California 95035, USA.
  • Bautista MJ; Nanosys, Inc., 233 S. Hillview Dr., Milpitas, California 95035, USA.
  • Ippen C; Nanosys, Inc., 233 S. Hillview Dr., Milpitas, California 95035, USA.
  • Ma R; Nanosys, Inc., 233 S. Hillview Dr., Milpitas, California 95035, USA.
  • Kelley AM; Chemistry and Biochemistry, University of California Merced, 5200 North Lake Road, Merced, California 95343, USA.
  • Kelley DF; Chemistry and Biochemistry, University of California Merced, 5200 North Lake Road, Merced, California 95343, USA.
J Chem Phys ; 155(24): 244705, 2021 Dec 28.
Article em En | MEDLINE | ID: mdl-34972380
ABSTRACT
We have used time-correlated single photon counting to elucidate the radiative dynamics of InP/ZnSe/ZnS core/shell/shell quantum dots (QDs) that differ in the amount and distribution of excess indium. Stoichiometric QDs having an InP atom ratio very near unity exhibit simple luminescence kinetics. The photoluminescence (PL) rises with the 40 ps instrument response function and exhibits a decay that is close to a single exponential with a time constant that decreases from 32 to 28 ns with increasing shell thickness. QDs having excess indium (InP ratio of 1.15-1.63) show a significant component of a slower rise time assigned to transient population of indium-based hole traps in the ZnSe shell. They also have a slower PL decay, attributed to an equilibrium between these traps, which are optically dark, and the emissive valence-band state. This results in a radiative lifetime that increases from 32 to 48 ns with increasing shell thickness. Different treatments of the InP cores prior to shell deposition result in different core/shell interfaces as indicated by resonance Raman spectroscopy, as well as differences in the amplitude and timescale of the slow PL rise and the PL decay time. These are interpreted in terms of different radial distributions of the indium-based hole traps, which can be related to differences in the interfacial lattice strain.