Investigating Influences of Synthesizing Eco-Friendly Waste-Coir-Fiber Nanofiller-Based Ramie and Abaca Natural Fiber Composite Parameters on Mechanical Properties.
Sathish, T; Mohanavel, Vinayagam; Velmurugan, Palanivel; Saravanan, R; Raja, T; Ravichandran, M; Alonazi, Wadi B; Sureshkumar, Shanmugam; Gebrekidan, Atkilt Mulu.
Afiliação
  • Sathish T; Department of Mechanical Engineering, Saveetha School of Engineering, SIMATS, Chennai 602 105, Tamil Nadu, India.
  • Mohanavel V; Centre for Materials Engineering and Regenerative Medicine, Bharath Institute of Higher Education and Research, Selaiyur, Chennai 600073, Tamil Nadu, India.
  • Velmurugan P; Centre for Materials Engineering and Regenerative Medicine, Bharath Institute of Higher Education and Research, Selaiyur, Chennai 600073, Tamil Nadu, India.
  • Saravanan R; Department of Mechanical Engineering, Saveetha School of Engineering, SIMATS, Chennai 602 105, Tamil Nadu, India.
  • Raja T; Department of Mechanical Engineering, Vel Tech Rangarajan Dr. Sakunthala R&D Institute of Science and Technology, Chennai 600062, India.
  • Ravichandran M; Department of Mechanical Engineering, K. Ramakrishnan College of Engineering, Trichy 621112, Tamil Nadu, India.
  • Alonazi WB; Health Administration Department, College of Business Administration, King Saud University, PO Box 71115, Riyadh 11587, Saudi Arabia.
  • Sureshkumar S; Department of Animal Resources Science, Dankook University, 119,Dandae-ro, Cheonan,31116, Republic of Korea.
  • Gebrekidan AM; Department of Mechanical Engineering, Faculty of Mechanical Engineering, Arba Minch Institute of Technology (AMIT), Arba Minch University, Addis Ababa, Ethiopia.
Bioinorg Chem Appl ; 2022: 6557817, 2022.
Article em En | MEDLINE | ID: mdl-35154295
Clean technology-based natural fiber composite fabrication is the prime aim of this piece of research. Natural fibers highly replace metal usage in industries and automobile, marine, medical applications, and so on. Vast amounts of natural fibers are freely available in all areas. In this research, work nanofiller material such as nano form waste coir fiber is collected from used car seat. The 10 wt.% of nanofiller material is added to the preparation of natural nanocomposites (ramie and abaca fiber). Hybrid composites are fabricated with the influence of different process parameters, namely, fiber weight percentage (20 wt.%, 30 wt.%, 40 wt.%, and 50 wt.%), NaOH action % (4%, 6%, 8%, and 10%), compression pressure (9 MPa, 12 MPa, 15 MPa, and 18 MPa), and temperature (100°C, 120°C, 140°C, and 160°C). Furthermore, the strength of this hybrid composite has analyzed by conducting flexural, impact, and shore hardness tests. These tests have provided the influence of selected parameters and their effects on the results of experimental work. In the flexural analysis, 6% of NaOH action has offered maximum flexural strength of the specimens. Correspondingly in the impact test, 30 wt.% of fiber is produced higher impact strength. Finally, applying 15 Mpa of compression pressure records the maximum shore hardness.