Your browser doesn't support javascript.
loading
Preparation and evaluation of molding-type solid-phase extraction media binding with commercially available adhesives.
Miki, Yuta; Murakami, Hiroya; Iida, Keisuke; Umemura, Tomonari; Esaka, Yukihiro; Inoue, Yoshinori; Teshima, Norio.
Afiliação
  • Miki Y; Department of Applied Chemistry, Aichi Institute of Technology, 1247 Yachigusa, Yakusa-cho, Toyota, 470-0392, Japan.
  • Murakami H; Department of Applied Chemistry, Aichi Institute of Technology, 1247 Yachigusa, Yakusa-cho, Toyota, 470-0392, Japan. hmurakami@aitech.ac.jp.
  • Iida K; Department of Applied Chemistry, Aichi Institute of Technology, 1247 Yachigusa, Yakusa-cho, Toyota, 470-0392, Japan.
  • Umemura T; School of Life Sciences, Tokyo University of Pharmacy and Life Sciences, 1432-1 Horinouchi, Hachioji, 192-0392, Japan.
  • Esaka Y; Gifu Pharmaceutical University, Daigaku-nishi, Gifu, 501-1196, Japan.
  • Inoue Y; Department of Applied Chemistry, Aichi Institute of Technology, 1247 Yachigusa, Yakusa-cho, Toyota, 470-0392, Japan.
  • Teshima N; Department of Applied Chemistry, Aichi Institute of Technology, 1247 Yachigusa, Yakusa-cho, Toyota, 470-0392, Japan.
Anal Sci ; 38(2): 307-315, 2022 02.
Article em En | MEDLINE | ID: mdl-35314976
ABSTRACT
A fabrication method of molding-type solid-phase extraction media (M-SPEM) bound with commercially available adhesive is presented. Six pieces of M-SPEM were prepared by heating each kneaded product of a particulate sorbent and an adhesive inserted into a six-hole cylindrical mold for hardening under an open system and normal pressure. The particulate sorbent contained in M-SPEM was divinylbenzene-based reversed-phase mode solid-phase extractants that we have reported. An examination of several adhesives showed that the moldability of M-SPEM depended on the composition and properties of the adhesive. The optimized procedure can be used to prepare an M-SPEM containing an 85 wt% particulate sorbent (particulate sorbent/adhesive, 100 mg/17 mg; particle diameter, 90-150 µm), and the M-SPEM has a specific surface area of about 500 m2/g. The established procedure in this study can bind particulate sorbents together, which showed almost no reductions in the adsorption property and liquid permeability compared with those of the particulate sorbent.
Assuntos
Palavras-chave

Texto completo: 1 Coleções: 01-internacional Base de dados: MEDLINE Assunto principal: Adesivos / Extração em Fase Sólida Idioma: En Ano de publicação: 2022 Tipo de documento: Article

Texto completo: 1 Coleções: 01-internacional Base de dados: MEDLINE Assunto principal: Adesivos / Extração em Fase Sólida Idioma: En Ano de publicação: 2022 Tipo de documento: Article