Activity-Stability Trends of the Sb-SnO2@RuOx Heterostructure toward Acidic Water Oxidation.
Park, Su-Young; An, Jung-Won; Baek, Ji-Hu; Woo, Hyun-Jae; Lee, Woo-Jae; Kwon, Se-Hun; Bera, Susanta.
Afiliação
  • Park SY; School of Materials Science and Engineering, Pusan National University, Busan 46241, Republic of Korea.
  • An JW; School of Materials Science and Engineering, Pusan National University, Busan 46241, Republic of Korea.
  • Baek JH; School of Materials Science and Engineering, Pusan National University, Busan 46241, Republic of Korea.
  • Woo HJ; School of Materials Science and Engineering, Pusan National University, Busan 46241, Republic of Korea.
  • Lee WJ; Institute of Materials Technology, Pusan National University, Busan 46241, Republic of Korea.
  • Kwon SH; School of Materials Science and Engineering, Pusan National University, Busan 46241, Republic of Korea.
  • Bera S; Institute of Materials Technology, Pusan National University, Busan 46241, Republic of Korea.
ACS Appl Mater Interfaces ; 15(12): 15332-15343, 2023 Mar 29.
Article em En | MEDLINE | ID: mdl-36940264
Accomplishments of enhanced activity and durability are a major concern in the design of catalysts for acidic water oxidation. To date, most studied supported metal catalysts undergo fast degradation in strongly acidic and oxidative environments due to improper controlling of the interface stability caused by their lattice mismatches. Here, we evaluate the activity-stability trends of in situ crystallized antimony-doped tin oxide (Sb-SnO2)@RuOx (Sb-SnO2@RuOx) heterostructure nanosheets (NSs) for acidic water oxidation. The catalyst prepared by atomic layer deposition of a conformal Ru film on antimony-doped tin sulfide (Sb-SnS2) NSs followed by heat treatment highlights comparable activity but longer stability than that of the ex situ catalyst (where Ru was deposited on Sb-SnO2 followed by heating). Air calcination for in situ crystallization allows the formation of hierarchical mesoporous Sb-SnO2 NSs from as-prepared Sb-SnS2 NSs and parallel in situ transformation from Ru to RuOx, resulting in a compact heterostructure. The significance of this approach significantly resists corrosive dissolution, which is justified by the enhanced oxygen evolution reaction (OER) stability of the catalyst compared to most of the state-of-the-art ruthenium-based catalysts including Carbon@RuOx (which shows ∼10 times higher dissolution) as well as Sb-SnO2@Com. RuOx and Com. RuO2. This study demonstrates the controlled interface stability of heterostructure catalysts toward enhancing OER activity and stability.