Your browser doesn't support javascript.
loading
First-principles evaluation of dopant impact on structural deformability and processability of Li7La3Zr2O12.
Dive, A; Kim, K; Kang, S; Wan, L F; Wood, B C.
Afiliação
  • Dive A; Laboratory for Energy Applications for the Future (LEAF), Materials Science Division, Lawrence Livermore National Laboratory, Livermore, California 94551-0808, USA. aniruddha.dive@wsu.edu.
  • Kim K; Laboratory for Energy Applications for the Future (LEAF), Materials Science Division, Lawrence Livermore National Laboratory, Livermore, California 94551-0808, USA. aniruddha.dive@wsu.edu.
  • Kang S; Laboratory for Energy Applications for the Future (LEAF), Materials Science Division, Lawrence Livermore National Laboratory, Livermore, California 94551-0808, USA. aniruddha.dive@wsu.edu.
  • Wan LF; Laboratory for Energy Applications for the Future (LEAF), Materials Science Division, Lawrence Livermore National Laboratory, Livermore, California 94551-0808, USA. aniruddha.dive@wsu.edu.
  • Wood BC; Laboratory for Energy Applications for the Future (LEAF), Materials Science Division, Lawrence Livermore National Laboratory, Livermore, California 94551-0808, USA. aniruddha.dive@wsu.edu.
Phys Chem Chem Phys ; 2023 Jul 19.
Article em En | MEDLINE | ID: mdl-37464810
ABSTRACT
Li7La3Zr2O12 (LLZO) and related ceramic solid electrolytes feature excellent stability and reasonable ionic conductivity, but processing remains challenging. High-temperature co-sintering is required for successful integration with the electrode, which is energetically costly and can lead to unacceptable cathode degradation. The introduction of dopants can promote lower-temperature processing by improving deformability and disrupting lattice integrity; however, an unbiased, systematic study correlating these properties to the dopant chemistry and composition is lacking. Here, we rely on a set of static and dynamic metrics derived from first-principles simulations to estimate the impact of doping on LLZO processability by quantifying LLZO structural deformability. We considered three distinct dopants (Al, Ba, and Ta) as representatives of substitutional incorporation on Li, La, and Zr sites. Our descriptors indicate that doping in general positively impacts lattice deformability, although significant sensitivities to dopant identity and concentration are observed. Amongst the tested dopants, Al doping (on the Li site) appears to have the greatest impact, as signaled across nearly the entire set of computed features. We suggest that these proxy descriptors, once properly calibrated against well-controlled experiments, could enable the use of first-principles simulations to computationally screen new ceramic electrolyte compositions with improved processability.