Your browser doesn't support javascript.
loading
Non-Electroconductive Polymer Coating on Graphite Mitigating Electrochemical Degradation of PTFE for a Dry-Processed Lithium-Ion Battery Anode.
Lee, Taegeun; An, Jiwoo; Chung, Woo Jun; Kim, Hyuntae; Cho, Yongil; Song, Hannah; Lee, Hyeonha; Kang, Jong Hun; Choi, Jang Wook.
Afiliação
  • Lee T; School of Chemical and Biological Engineering and the Institute of Chemical Processes, Seoul National University, 1 Gwanak-ro, Gwanak-gu, Seoul 08826, Republic of Korea.
  • An J; School of Chemical and Biological Engineering and the Institute of Chemical Processes, Seoul National University, 1 Gwanak-ro, Gwanak-gu, Seoul 08826, Republic of Korea.
  • Chung WJ; School of Chemical and Biological Engineering and the Institute of Chemical Processes, Seoul National University, 1 Gwanak-ro, Gwanak-gu, Seoul 08826, Republic of Korea.
  • Kim H; School of Chemical and Biological Engineering and the Institute of Chemical Processes, Seoul National University, 1 Gwanak-ro, Gwanak-gu, Seoul 08826, Republic of Korea.
  • Cho Y; Battery Manufacturing Engineering R&D Team, Kia Corporation, 37 Cheoldobangmulgwan-ro, Uiwang-si 16082, Gyeonggi-do, Republic of Korea.
  • Song H; Battery Manufacturing Engineering R&D Team, Hyundai Motor Company, 37 Cheoldobangmulgwan-ro, Uiwang-si 16082, Gyeonggi-do, Republic of Korea.
  • Lee H; Battery Manufacturing Engineering R&D Team, Kia Corporation, 37 Cheoldobangmulgwan-ro, Uiwang-si 16082, Gyeonggi-do, Republic of Korea.
  • Kang JH; School of Chemical and Biological Engineering and the Institute of Chemical Processes, Seoul National University, 1 Gwanak-ro, Gwanak-gu, Seoul 08826, Republic of Korea.
  • Choi JW; School of Chemical and Biological Engineering and the Institute of Chemical Processes, Seoul National University, 1 Gwanak-ro, Gwanak-gu, Seoul 08826, Republic of Korea.
ACS Appl Mater Interfaces ; 16(7): 8930-8938, 2024 Feb 21.
Article em En | MEDLINE | ID: mdl-38326747
ABSTRACT
Polytetrafluoroethylene (PTFE)-based dry process for lithium-ion batteries is gaining attention as a battery manufacturing scheme can be simplified with drastically reducing environmental damage. However, the electrochemical instability of PTFE in a reducing environment has hampered the realization of the high-performance dry-processed anode. In this study, we present a non-electroconductive and highly ionic-conductive polymer coating on graphite to mitigate the electrochemical degradation of the PTFE binder and minimize the coating resistance. Poly(ethylene oxide) (PEO) and poly(vinylidene fluoride-trifluoroethylene-chlorofluoroethylene) (P(VDF-TrFE-CFE)) coatings on the anode material effectively inhibit the electron transfer from graphite to PTFE, thereby alleviating the PTFE breakdown. The graphite polymer coatings improved initial Coulombic efficiencies of full cells from 67.2% (bare) to 79.1% (PEO) and 77.8% (P(VDF-TrFE-CFE)) and increased initial discharge capacity from 157.7 mAh g(NCM)-1 (bare) to 185.1 mAh g(NCM)-1 (PEO) and 182.5 mAh g(NCM)-1 (P(VDF-TrFE-CFE)) in the full cells. These outcomes demonstrate that PTFE degradation in the anode can be surmounted by adjusting the electron transfer to the PTFE.