The swelling behaviors and water retention of superabsorbent materials prepared from acrylic acid/acrylamide copolymer and acid-modified attapulgite under ultrasonic treatment and different pH conditions were investigated. The results demonstrated that a suitable amount of attapulgite can effectively improve the absorption capacity. The superabsorbent achieved the highest absorptions of 1257.54 g g-1 and 209.45 g g-1 in distilled water and a 0.9 wt% NaCl solution, and a higher water absorbency occurred over a wide pH range of 5-9 when the ultrasonic power was 200 W, and the attapulgite content was 10%. Addition of attapulgite could significantly increase the water absorption and retention of this kind of material, which can be applied as a sand-fixing material.
Texto completo:
1
Coleções:
01-internacional
Base de dados:
MEDLINE
Idioma:
En
Ano de publicação:
2024
Tipo de documento:
Article