Your browser doesn't support javascript.
loading
Microtensile bond strength of CAD/CAM materials to dentin under different adhesive strategies
Bellan, Mariá Cortina; Cunha, Patrícia Fernandes Jerzewski Sotero da; Tavares, Julieta Gomes; Spohr, Ana Maria; Mota, Eduardo Gonçalves.
  • Bellan, Mariá Cortina; Pontifícia Universidade Católica da Universidade Federal do Rio Grande do Sul - PUC-RS. School of Dentistry. Porto Alegre. BR
  • Cunha, Patrícia Fernandes Jerzewski Sotero da; São Leopoldo Mandic. School of Dentistry. Porto Alegre. BR
  • Tavares, Julieta Gomes; Pontifícia Universidade Católica da Universidade Federal do Rio Grande do Sul - PUC-RS. School of Dentistry. Porto Alegre. BR
  • Spohr, Ana Maria; Pontifícia Universidade Católica da Universidade Federal do Rio Grande do Sul - PUC-RS. School of Dentistry. Porto Alegre. BR
  • Mota, Eduardo Gonçalves; Pontifícia Universidade Católica da Universidade Federal do Rio Grande do Sul - PUC-RS. School of Dentistry. Porto Alegre. BR
Braz. oral res. (Online) ; 31: e109, 2017. tab, graf
Article in English | LILACS | ID: biblio-952095
ABSTRACT
Abstract The present study aimed to evaluate the microtensile bond strength (μTBS) of novel computer-aided design/computer-aided manufacturing (CAD/CAM) restorative materials to dentin using different adhesive strategies. Thirty-two crowns were milled using CAD/CAM materials (Vita Mark II as control, Vita Suprinity, Vita Enamic and Lava Ultimate) and luted to dentin using different resin cements (RelyX ARC, RelyX Unicem 2 and RelyX Ultimate). The specimens were stored in 100% relative humidity at 37°C for 24 h and sectioned. The samples (n = 16) with cross-sectional areas of approximately 0.90 mm2, were submitted to a μTBS test in a universal testing machine with a crosshead speed of 0.5 mm/min. The samples were analyzed with SEM to determinate the failure mode. According to 2-way ANOVA and Tukey's test (α=0.05), the interaction effect (material x luting strategy) was significant (p=0.001). Regardless of the luting strategy, a higher μTBS was obtained with Lava Ultimate and Vita Enamic, which were significantly different from Vita Mark II and Vita Suprinity (p<0.05). For Vita Mark II, Vita Suprinity, Vita Enamic, and Lava Ultimate, the μTBS obtained with RelyX Unicem 2 was not significantly different from that obtained with RelyX ARC or RelyX Ultimate. All groups obtained at least three types of failure. The adhesive strategy with self-adhesive resin cement was comparable to conventional resin cement with total-etch or self-etch adhesive techniques in the bond of novel CAD/CAM materials to dentin.
Subject(s)


Full text: Available Index: LILACS (Americas) Main subject: Ceramics / Dental Bonding / Computer-Aided Design / Resin Cements / Dentin Type of study: Evaluation studies Limits: Humans Language: English Journal: Braz. oral res. (Online) Journal subject: Dentistry Year: 2017 Type: Article Affiliation country: Brazil Institution/Affiliation country: Pontifícia Universidade Católica da Universidade Federal do Rio Grande do Sul - PUC-RS/BR / São Leopoldo Mandic/BR

Similar

MEDLINE

...
LILACS

LIS


Full text: Available Index: LILACS (Americas) Main subject: Ceramics / Dental Bonding / Computer-Aided Design / Resin Cements / Dentin Type of study: Evaluation studies Limits: Humans Language: English Journal: Braz. oral res. (Online) Journal subject: Dentistry Year: 2017 Type: Article Affiliation country: Brazil Institution/Affiliation country: Pontifícia Universidade Católica da Universidade Federal do Rio Grande do Sul - PUC-RS/BR / São Leopoldo Mandic/BR