Nanotoxicology ; 6(6): 587-99, 2012 Sep.
Artigo em Inglês | MEDLINE | ID: mdl-21714591

RESUMO

Multi-walled carbon nanotubes (MWCNTs), dispersed in suspensions consisting mainly of individual tubes, were used for intratracheal instillation and inhalation studies. Rats intratracheally received a dose of 0.2 mg, or 1 mg of MWCNTs and were sacrificed from 3 days to 6 months. MWCNTs induced a pulmonary inflammation, as evidenced by a transient neutrophil response in the low-dose groups, and presence of small granulomatous lesion and persistent neutrophil infiltration in the high-dose groups. In the inhalation study, rats were exposed to 0.37 mg/m(3) aerosols of well-dispersed MWCNTs (>70% of MWCNTs were individual fibers) for 4 weeks, and were sacrificed at 3 days, 1 month, and 3 months after the end of exposure. The inhalation exposures delivered less amounts of MWCNTs into the lungs, and therefore less pulmonary inflammation responses was observed, as compared to intratracheal instillation. The results of our study show that well-dispersed MWCNT can produce pulmonary lesions, including inflammation.


Assuntos
Pulmão/efeitos dos fármacos , Nanotubos de Carbono/toxicidade , Administração por Inalação , Fosfatase Alcalina/metabolismo , Animais , Líquido da Lavagem Broncoalveolar/química , Líquido da Lavagem Broncoalveolar/citologia , Quimiocinas CXC/análise , Quimiocinas CXC/metabolismo , Pulmão/química , Pulmão/patologia , Macrófagos Alveolares/efeitos dos fármacos , Macrófagos Alveolares/patologia , Masculino , Nanotubos de Carbono/química , Peroxidase/metabolismo , Ratos , Ratos Wistar , Estatísticas não Paramétricas , Testes de Toxicidade
2.
Inhal Toxicol ; 23(13): 784-91, 2011 Nov.
Artigo em Inglês | MEDLINE | ID: mdl-22035120

RESUMO

It is important to conduct a risk assessment that includes hazard assessment and exposure assessment for the safe production and handling of newly developed nanomaterials. We conducted an inhalation study of a multi-wall carbon nanotube (MWCNT) as a hazard assessment. Male Wistar rats were exposed to well-dispersed MWCNT for 4 weeks by whole body inhalation. The exposure concentration in the chamber was 0.37 ± 0.18 mg/m³. About 70% of the MWCNTs in the chamber were single fiber. The geometric mean diameter (geometric standard deviation, GSD) and geometric mean length (GSD) of the aerosolized MWCNTs in the chamber were 63 nm (1.5) and 1.1 µm (2.7), respectively. The amounts of MWCNT deposited in the rat lungs were determined by the X-ray diffraction method and elemental carbon analysis. The average deposited amounts at 3 days after the inhalation were 68 µg/lung by the X-ray diffraction method and 76 µg/lung by elemental carbon analysis. The calculated deposition fractions were 18% and 20% in each analysis. The amount of retained MWCNT in the lungs until 3 months after the inhalation decreased exponentially and the calculated biological half times of MWCNT were 51 days and 54 days, respectively. The clearance was not delayed, but a slight increase in lung weight at 3 days after the inhalation was observed.


Assuntos
Pulmão/metabolismo , Nanotubos de Carbono , Administração por Inalação , Animais , Pulmão/patologia , Masculino , Ratos , Ratos Wistar , Distribuição Tecidual , Testes de Toxicidade Subaguda , Difração de Raios X
3.
Talanta ; 84(3): 802-8, 2011 May 15.
Artigo em Inglês | MEDLINE | ID: mdl-21482285

RESUMO

This paper describes a method for determination of multiwall carbon nanotubes (MWCNTs) in rat lungs after intratracheal instillation exposure. The MWCNTs were quantitatively decomposed to CO(2) by combustive oxidation and were then determined by non-dispersive infrared analysis. Samples were pretreated by acid digestion, muffle ashing and in situ preheating to remove interferences due to coexisting biological carbon from the lung tissue sample, while preserving the MWCNTs as in its their original form. The preservation was confirmed by transmission electron microscopic observation of the pretreated samples of exposed lung tissues and by the fact that the recoveries of MWCNTs spiked to the lung tissues were close to 100%. The detection limit for MWCNTs obtained by the proposed method was 0.30 µg and the repeatability as expressed by the relative standard deviation was 5.6% (n=4). The method was sufficiently sensitive and precise to apply to real samples of rat lung to investigate the in vivo persistence of intratracheally instilled MWCNTs. To our knowledge, this is the first report of this type of sample pretreatment and direct determination of pristine MWCNTs without modification or tagging. Conventional indirect methods use tagging with other compounds or metal impurities in the CNTs for detection, and the detachment of these tags can increase uncertainties in the determination of the CNTs. The tags can also change how the CNTs persist in vivo, which can lead to an incorrect understanding of the persistence of pristine CNTs in vivo.


Assuntos
Pulmão/metabolismo , Nanotubos de Carbono , Traqueia , Animais , Vias de Administração de Medicamentos , Limite de Detecção , Microscopia Eletrônica de Transmissão , Oxirredução , Ratos