Topotactic phase transformation enables structural transition without losing the crystalline symmetry of the parental phase and provides an effective platform for elucidating the redox reaction and oxygen diffusion within transition metal oxides. In addition, it enables tuning of the emergent physical properties of complex oxides, through strong interaction between the lattice and electronic degrees of freedom. In this communication, the electronic structure evolution of SrFeOx epitaxial thin films is identified in real-time, during the progress of reversible topotactic phase transformation. Using real-time optical spectroscopy, the phase transition between the two structurally distinct phases (i.e., brownmillerite and perovskite) is quantitatively monitored, and a pressure-temperature phase diagram of the topotactic transformation is constructed for the first time. The transformation at relatively low temperatures is attributed to a markedly small difference in Gibbs free energy compared to the known similar class of materials to date. This study highlights the phase stability and reversibility of SrFeOx thin films, which is highly relevant for energy and environmental applications exploiting the redox reactions.

2.
Phys Rev Lett ; 115(22): 226402, 2015 Nov 27.
Artigo em Inglês | MEDLINE | ID: mdl-26650312

RESUMO

Barium bismuth oxide (BaBiO_{3}) is the end member of two families of high-T_{c} superconductors, i.e., BaPb_{1-x}Bi_{x}O_{3} and Ba_{1-x}K_{x}BiO_{3}. The undoped parent compound is an insulator, exhibiting a charge density wave that is strongly linked to a static breathing distortion in the oxygen sublattice of the perovskite structure. We report a comprehensive spectroscopic and x-ray diffraction study of BaBiO_{3} thin films, showing that the minimum film thickness required to stabilize the breathing distortion and charge density wave is ≈11 unit cells, and that both phenomena are suppressed in thinner films. Our results constitute the first experimental observation of charge density wave suppression in bismuthate compounds without intentionally introducing dopants.