1.
Sci Adv ; 2(9): e1501814, 2016 09.
Artigo em Inglês | MEDLINE | ID: mdl-27652338

RESUMO

Relaxor-based ferroelectrics are prized for their giant electromechanical coupling and have revolutionized sensor and ultrasound applications. A long-standing challenge for piezoelectric materials has been to understand how these ultrahigh electromechanical responses occur when the polar atomic displacements underlying the response are partially broken into polar nanoregions (PNRs) in relaxor-based ferroelectrics. Given the complex inhomogeneous nanostructure of these materials, it has generally been assumed that this enhanced response must involve complicated interactions. By using neutron scattering measurements of lattice dynamics and local structure, we show that the vibrational modes of the PNRs enable giant coupling by softening the underlying macrodomain polarization rotations in relaxor-based ferroelectric PMN-xPT {(1 - x)[Pb(Mg1/3Nb2/3)O3] - xPbTiO3} (x = 30%). The mechanism involves the collective motion of the PNRs with transverse acoustic phonons and results in two hybrid modes, one softer and one stiffer than the bare acoustic phonon. The softer mode is the origin of macroscopic shear softening. Furthermore, a PNR mode and a component of the local structure align in an electric field; this further enhances shear softening, revealing a way to tune the ultrahigh piezoelectric response by engineering elastic shear softening.


Assuntos
Imãs/química , Fenômenos Mecânicos , Nanoestruturas/química , Fônons , Impedância Elétrica , Eletricidade , Microscopia de Força Atômica , Difração de Nêutrons , Titânio/química , Vibração
2.
J Appl Phys ; 114(10): 104505, 2013 Sep 14.
Artigo em Inglês | MEDLINE | ID: mdl-24143033

RESUMO

The most difficult task in the characterization of complete set material properties for piezoelectric materials is self-consistency. Because there are many independent elastic, dielectric, and piezoelectric constants, several samples are needed to obtain the full set constants. Property variation from sample to sample often makes the obtained data set lack of self-consistency. Here, we present a method, based on pulse-echo ultrasound and inverse impedance spectroscopy, to precisely determine the full set physical properties of piezoelectric materials using only one small sample, which eliminated the sample to sample variation problem to guarantee self-consistency. The method has been applied to characterize the [001]C poled Mn modified 0.27Pb(In1/2Nb1/2)O3-0.46Pb(Mg1/3Nb2/3)O3-0.27PbTiO3 single crystal and the validity of the measured data is confirmed by a previously established method. For the inverse calculations using impedance spectrum, the stability of reconstructed results is analyzed by fluctuation analysis of input data. In contrast to conventional regression methods, our method here takes the full advantage of both ultrasonic and inverse impedance spectroscopy methods to extract all constants from only one small sample. The method provides a powerful tool for assisting novel piezoelectric materials of small size and for generating needed input data sets for device designs using finite element simulations.

3.
J Appl Phys ; 113(7): 74106, 2013 Feb 21.
Artigo em Inglês | MEDLINE | ID: mdl-23509414

RESUMO

Mn modified rhombohedral Pb(In0.5Nb0.5)O3-Pb(Mg1/3Nb2/3)O3-PbTiO3 (PIN-PMN-PT:Mn) single crystals poled along [011]C crystallographic direction exhibit a "2R" engineered domain configuration, with macroscopic mm2 symmetry. The complete sets of material constants were determined using combined resonance and ultrasonic methods, and compared to [001]C poled PIN-PMN-PT:Mn crystals. The thickness shear piezoelectric coefficient d15 and electromechanical coupling factor k15 were found to be on the order of ∼3000 pC/N and 0.92, respectively, with longitudinal piezoelectric coefficient d33 and coupling factor k33 being on the order of ∼1050 pC/N and 0.90. Of particular importance is that PIN-PMN-PT:Mn single crystals exhibited high mechanical quality factor Q33 ∼ 1000, comparable to "hard" PZT8 ceramics, which can also be confirmed by the low extrinsic contribution, being ≤2% from the Rayleigh analysis.

4.
Artigo em Inglês | MEDLINE | ID: mdl-25004527

RESUMO

Piezoelectric materials lie at the heart of electromechanical devices. Applications include actuators, ultrasonic imaging, high intensity focused ultrasound, underwater ultrasound, nondestructive evaluation transducer, pressure sensors, and accelerometers, to name a few. In this work, the advantages and disadvantages of relaxor-PbTiO(3)-based single crystals are discussed, based on the requirements (figure of merit) of various applications, with emphasis on recent developments of the shear properties of single crystals as a function of temperature and applied fields.


Assuntos
Cristalização/métodos , Chumbo/química , Chumbo/efeitos da radiação , Sistemas Microeletromecânicos/instrumentação , Titânio/química , Titânio/efeitos da radiação , Transdutores , Ultrassonografia/instrumentação , Desenho de Equipamento , Ondas de Choque de Alta Energia , Teste de Materiais , Espalhamento de Radiação
5.
J Appl Phys ; 112(12): 124113, 2012 Dec 15.
Artigo em Inglês | MEDLINE | ID: mdl-23341689

RESUMO

Mn modified 0.26Pb(In(1/2)Nb(1/2))O(3)-0.42Pb(Mg(1/3)Nb(2/3))O(3)-0.32PbTiO(3) (PIN-PMN-PT:Mn) single crystals with orthorhombic perovskite crystal structure were polarized along [011] direction, resulting in the single domain state "1O." The complete set of material constants was determined using the combined resonance and ultrasonic methods. The thickness shear piezoelectric coefficient d(15) and electromechanical coupling factor k(15) were found to be on the order of 3100 pC/N and 94%, respectively, much higher than longitudinal d(33) ∼ 270 pC/N and k(33) ∼ 70%. Using the single domain data, the rotated value of d(33)* along [001] direction was found to be 1230 pC/N, in agreement with the experimentally determined d(33) value of 1370 pC/N, conferring extrinsic contributions being about 10%, which was also confirmed using the Rayleigh analysis. In addition, the mechanical quality factors Q(m) were evaluated for different "1O" vibration modes, where the longitudinal Q(m) was found to be ∼1200, much higher than the value for "4O" crystals, ∼300.