Int J Biol Macromol ; 161: 927-935, 2020 Oct 15.
Artigo em Inglês | MEDLINE | ID: mdl-32531359

RESUMO

Incorporation of drugs in clay minerals has been widely proposed for the controlled-release or increased solubility of drugs. In this context, a bionanocomposite based on kaolinite and cashew gum (Kln/Gum) was synthesized and characterized by X-ray diffraction (XRD), thermal analysis (TG/DTA), and Fourier transform infrared spectroscopy (FTIR). The bionanocomposite was applied to the incorporation and further release of doxazosin mesylate (DB). The influence of solution pH (1-3), adsorbent dose (20-50 mg), initial drug concentration (20.0-70.0 mg L-1), contact time (15-300 min), and temperature (25, 35, and 45 °C) were systematically evaluated. Equilibrium was reached around 60 min, with a maximum adsorption capacity of 31.5 ± 2.0 mg g-1 at a pH of 3.0 and 25 °C. Hydrogen bonding contributed to DB incorporation on the Kln/Gum. In addition, DB maximum amounts of 16.80 ± 0.58 and 77.00 ± 2.46% were released at pH values of 1.2 and 7.4, respectively. These results indicated that the Kln/Gum bionanocomposite is an effective and promising material for the incorporation/release of drugs with similar structures to DB.


Assuntos
Anacardium/química , Doxazossina/química , Gengiva/química , Caulim/química , Nanocompostos/química , Adsorção , Argila/química , Concentração de Íons de Hidrogênio , Minerais/química , Espectroscopia de Infravermelho com Transformada de Fourier/métodos , Temperatura , Difração de Raios X/métodos
SELEÇÃO DE REFERÊNCIAS
DETALHE DA PESQUISA
...