Surface and mechanical properties of adhesives with calcium phosphates challenged to different storage media
Gómez, Marcelo Matias Mederos; Garcia, Isadora Martini; Leitune, Vicente Castelo Branco; Collares, Fabrício Mezzomo.
Afiliação
  • Gómez, Marcelo Matias Mederos; University of the Republic. Faculty of Dentistry. Department of Montevideo. Montevideo. UY
  • Garcia, Isadora Martini; Federal University of Rio Grande do Sul. School of Dentistry. Department of Dental Materials. Porto Alegre. BR
  • Leitune, Vicente Castelo Branco; Federal University of Rio Grande do Sul. School of Dentistry. Department of Dental Materials. Porto Alegre. BR
  • Collares, Fabrício Mezzomo; Federal University of Rio Grande do Sul. School of Dentistry. Department of Dental Materials. Porto Alegre. BR
Braz. j. oral sci ; 19: e200181, jan.-dez. 2020. ilus
Artigo em Inglês | BBO - Odontologia, LILACS | ID: biblio-1152205
Biblioteca responsável: BR218.1
ABSTRACT

Aim:

To evaluate the behavior of experimental dental adhesives with hydroxyapatite (HAp), alpha-tricalcium phosphate (α-TCP) or octacalcium phosphate (OCP) after storing them in three different media dry storage, distilled water, or lactic acid.

Methods:

An experimental adhesive resin was formulated with bisphenol A glycol dimethacrylate, 2-hydroxyethyl methacrylate, and photoiniciator/co-initiator system. HAp(GHAp), α-TCP (Gα-TCP), or OCP (GOCP) were added to the adhesive resin at 2 wt.%, and one group remained without calcium phosphates to be used as a control (GCtrl). The adhesives were evaluated for surface roughness, scanning electron microscopy (SEM), and ultimate tensile strength (UTS) after storing in distilled water (pH=5.8), lactic acid (pH=4) or dry medium.

Results:

The initial surface roughness was not different among groups (p>0.05). GHAp showed increased values after immersion in water (p<0.05) or lactic acid (p<0.05). SEM analysis showed a surface variation of the filled adhesives, mainly for Gα-TCP and GHAp. GHApshowed the highest UTS in dry medium (p<0.05), and its value decreased after lactic acid storage (p<0.05).

Conclusions:

The findings of this study showed that HAp, OCP, and α-TCP affected the physical behavior of the experimental adhesive resins in different ways. HAp was the calcium phosphate that most adversely affected the surface roughness and the mechanical property of the material, mainly when exposed to an acid medium
Assuntos


Texto completo: Disponível Coleções: Bases de dados internacionais Base de dados: BBO - Odontologia / LILACS Assunto principal: Polímeros / Resistência à Tração / Ácidos / Fosfatos de Cálcio / Adesivos Dentinários Idioma: Inglês Revista: Braz. j. oral sci Assunto da revista: Odontologia Ano de publicação: 2020 Tipo de documento: Artigo País de afiliação: Brasil / Uruguai Instituição/País de afiliação: Federal University of Rio Grande do Sul/BR / University of the Republic/UY

Texto completo: Disponível Coleções: Bases de dados internacionais Base de dados: BBO - Odontologia / LILACS Assunto principal: Polímeros / Resistência à Tração / Ácidos / Fosfatos de Cálcio / Adesivos Dentinários Idioma: Inglês Revista: Braz. j. oral sci Assunto da revista: Odontologia Ano de publicação: 2020 Tipo de documento: Artigo País de afiliação: Brasil / Uruguai Instituição/País de afiliação: Federal University of Rio Grande do Sul/BR / University of the Republic/UY
...