Your browser doesn't support javascript.
loading
Effects of three silane primers and five adhesive agents on the bond strength of composite material for a computer-aided design and manufacturing system
Shinohara, Ayano; Taira, Yohsuke; Sakihara, Michino; Sawase, Takashi.
Afiliação
  • Shinohara, Ayano; Nagasaki University. Graduate School of Biomedical Sciences. Department of Applied Prosthodontics. JP
  • Taira, Yohsuke; Nagasaki University. Graduate School of Biomedical Sciences. Department of Applied Prosthodontics. JP
  • Sakihara, Michino; Nagasaki University. Graduate School of Biomedical Sciences. Department of Applied Prosthodontics. JP
  • Sawase, Takashi; Nagasaki University. Graduate School of Biomedical Sciences. Department of Applied Prosthodontics. JP
J. appl. oral sci ; 26: e20170342, 2018. tab, graf
Artigo em Inglês | LILACS, BBO - Odontologia | ID: biblio-893688
Biblioteca responsável: BR1.1
ABSTRACT
Abstract Objective The objective of this study was to evaluate the effects of combinations of silane primers and adhesive agents on the bond strength of a composite block for a computer-aided design and manufacturing system. Material and Methods Three silane primers [Clearfil Ceramic Primer (CP), Super-Bond PZ Primer (PZ), and GC Ceramic Primer II (GP)] were used in conjunction with five adhesive agents [G-Premio Bond (P-Bond), Repair Adhe Adhesive (R-Adhesive), Super-Bond D-Liner Dual (SB-Dual), Super-Bond C&B (SB-Self), and SB-Dual without tributylborane derivative (SB-Light)]. The surface of a composite block (Gradia Block) was ground with silicon carbide paper. After treatment with a silane primer, a adhesive agent was applied to each testing specimen. The specimens were then bonded with a light-curing resin composite. After 24 h, the shear bond strength values were determined and compared using a post hoc test (α=0.05, n=8/group). We also prepared control specimens without primer (No primer) and/or without adhesive agent (No adhesive). Results PZ/SB-Dual and GP/SB-Dual presented the highest bond strength, followed by GP/P-Bond, CP/SB-Dual, CP/R-Adhesive, No primer/SB-Dual, GP/R-Adhesive, CP/P-Bond, No primer/R-Adhesive, PZ/R-Adhesive, CP/SB-Self, PZ/P-Bond, PZ/SB-Self, and GP/SB-Self in descending order of bond strength. No primer/P-Bond, No primer/SB-Self, and all specimens in the SB-Light and No adhesive groups presented the lowest bond strengths. Conclusion A dual-curing adhesive agent (SB-Dual) containing a tributylborane derivative in combination with a silane primer (GP or PZ) presents a greater bond strength between the composite block and the repairing resin composite than the comparators used in the study.
Assuntos


Texto completo: Disponível Coleções: Bases de dados internacionais Base de dados: BBO - Odontologia / LILACS Assunto principal: Silanos / Colagem Dentária / Resinas Compostas / Cimentos Dentários Idioma: Inglês Revista: J. appl. oral sci Assunto da revista: Odontologia Ano de publicação: 2018 Tipo de documento: Artigo País de afiliação: Japão Instituição/País de afiliação: Nagasaki University/JP

Texto completo: Disponível Coleções: Bases de dados internacionais Base de dados: BBO - Odontologia / LILACS Assunto principal: Silanos / Colagem Dentária / Resinas Compostas / Cimentos Dentários Idioma: Inglês Revista: J. appl. oral sci Assunto da revista: Odontologia Ano de publicação: 2018 Tipo de documento: Artigo País de afiliação: Japão Instituição/País de afiliação: Nagasaki University/JP
...