RESUMO
Objetivo:
Avaliar o efeito do clareamento dental sobre a resistência adesiva ao esmalte.Métodos:
Foram selecionados cinqüenta molares, os quais foram divididos aleatoriamente em cinco grupos (n=10); G1-sem clareamento (controle); G2-clareado com peróxido de carbamida a 10% e restaurado 24h após; G3-clareado com peróxido de carbamida a 10%e restaurado sete dias após; G4-clareado com peróxido de hidrogênio a 35% e restaurado 24h após; G5-clareado com peróxido de hidrogênio a 35% e restaurado sete dias após. Durante os intervalos de 24h e sete dias os corpos-de-prova ficaram armazenados em saliva artificial, quando então foram executados os procedimentos restauradores sobre o esmalte.Resultados:
O ensaio de resistência adesiva por microcisalhamento indicou os seguintes resultados em MPa (ANOVA e Tukey poste-hoc)G1-43,15 a (±5,19); G2-31,34 ab (± 4,41); G3-36,66 ab (± 3,11); G4-22,87 c (±3,76) e G5-35,67 ab (± 4,64).Conclusão:
Os grupos G1, G2, G3 e G5 não tiveram diferença estatística e o grupo G4 (clareado com peróxido de hidrogênio a 35% e restaurado 24 após) teve sua resistência adesiva entre o esmalte clareado e a resina composta diminuída.ABSTRACT
Objective:
To evaluate the effect of dental bleaching on the shear bond strength of enamel.Methods:
Fifty molars were selected and divided into five groups (n=10); G1-without bleaching (control); G2-bleached with 10% carbamide peroxide and restored 24h later; G3-bleached with 10% carbamide peroxide and restored seven days later; G4-bleached with 35%hydrogen peroxide and restored a 35% and restored 24h later; G5-bleached with 35% hydrogen peroxide and restored a 35% and restoredseven days later. During the 24h and 7-day intervals the test specimens remained stored in artificial saliva, after which the restorative procedures were performed on the enamel.Results:
The microshear bond strength test indicated the following results in MPa (ANOVA and Tukey post-hoc) G1-43.15 a (±5.19); G2-31.34 ab (± 4.41); G3-36.66 ab (± 3.11); G4-22.87 c (±3.76) and G5-35.67 ab (± 4.64).Conclusion:
Groups G1, G2, G3 and G5 showed no statistical difference and Group G4 (bleached with 35% hydrogen peroxide and restored 24h later) showed diminished bond strength between the bleached enamel and resin composite.Palavras-chave
Texto completo:
1
Coleções:
01-internacional
Base de dados:
LILACS
Assunto principal:
Clareamento Dental
/
Esmalte Dentário
/
Peróxido de Hidrogênio
Tipo de estudo:
Clinical_trials
/
Evaluation_studies
Limite:
Humans
Idioma:
Pt
Revista:
RGO (Porto Alegre)
Assunto da revista:
ODONTOLOGIA
Ano de publicação:
2008
Tipo de documento:
Article
País de afiliação:
Brasil
/
Estados Unidos
País de publicação:
Brasil