Your browser doesn't support javascript.
loading
Influência do tempo de armazenamento na resistência de união à microtração de diferentes sistemas adesivos em dentina superficial e profunda / Influence of water storage time on microtensile bond strength of different adhesive systems on superficial and deep dentin
Pupo, Yasmine Mendes; Martins, Gislaine Cristine; Gomes, Giovana Mongruel; Michél, Milton Domingos; Gomes, Osnara Maria Mongruel; Gomes, João Carlos.
Afiliação
  • Pupo, Yasmine Mendes; Universidade Estadual de Ponta Grossa. Ponta Grossa. BR
  • Martins, Gislaine Cristine; Universidade Estadual de Ponta Grossa. Ponta Grossa. BR
  • Gomes, Giovana Mongruel; Universidade Estadual de Ponta Grossa. Ponta Grossa. BR
  • Michél, Milton Domingos; Universidade Estadual de Ponta Grossa. Ponta Grossa. BR
  • Gomes, Osnara Maria Mongruel; Universidade Estadual de Ponta Grossa. Ponta Grossa. BR
  • Gomes, João Carlos; Universidade Estadual de Ponta Grossa. Ponta Grossa. BR
Braz. dent. sci ; 13(1/2): 16-22, 2010. tab
Artigo em Português | LILACS, BBO - Odontologia | ID: lil-642686
Biblioteca responsável: BR243.1
RESUMO
O objetivo deste estudo foi avaliar a resistência de união (RU) de um sistema adesivo convencional (Adper™ Single Bond 2 [SB] (3M ESPE, St. Paul, MN, EUA)) e de dois autocondicionantes (Adper™ SE Plus [SE] (3M ESPE, St. Paul, MN, EUA) e AdheSE® [AD] (Ivoclar Vivadent, Schaan, Liechtenstein, DDR)) em dentina superficial (DS) e profunda (DP), nos tempos imediatamente e após 6 meses de armazenamento em água. Superfícies oclusais de 24 terceiros molares humanos foram seccionadas e smear layer padronizada. Após procedimentos adesivos, as superfícies dos dentes receberam restaurações em resina composta. Tais dentes foram seccionados obtendo-se espécimes em forma de palitos (0,7 + 0,1mm2). Os espécimes foram testados por meio do ensaio de microtração (0,5 mm/min), imediatamente e após 6 meses de armazenamento em água. Os dados foram submetidos à ANOVA 3 fatores e ao pós-teste de Bonferroni (α=0,05). Na avaliação imediatamente da RU, apenas o fator “adesivo” foi significativo (p<0,05). Os dados de RU após 6 meses mostraram que a interação dos fatores “adesivo e substrato dentinário” foi significativa (p<0,05). AD em DS (IM 49,0 ± 6,7 MPa) mostrou diminuição significativa da RU após 6M (23,2 ± 7,9 MPa) de armazenamento em água. SE e AD mostraram diferença significativa (p<0,05) tanto em DS como em DP. Em DS o fator tempo foi significativo e em DP o fator adesivo foi significativo. SB tanto em DS como em DP não apresentou diferença estatisticamente significante imediatamente e após 6 meses (p>0,05). Conclui-se que diferentes níveis de profundidade dentinária podem afetar a RU para o mesmo material e que o fator tempo pode influenciar a degradação do sistema adesivo.
ABSTRACT
The aim of this study was to evaluate the resin-dentin bond strengths (μTBS) of a total-etch adhesive system (Adper™ Single Bond 2 [SB], 3M ESPE, St. Paul, MN, USA) and of two self-etch adhesive systems (Adper™ SE Plus [SE], 3M ESPE, St. Paul, MN, USA and AdheSE® [AD], Ivoclar Vivadent, Schaan, Liechtenstein, DDR) in superficial dentin (SD) and deep dentine (DD) immediately and after 6 months of storage in water. Surface occlusals of 24 carie-free human third molars were exposed to their SD or DD and polished to create a standardized smear layer. After the adhesive procedures, composite buildups were constructed incrementally and sectioned to obtain bonded sticks (0.7 + 0.1 mm2) that were tested in tension (0.5 mm/min) immediately and after 6 months of water storage. The μTBS data were submitted to a three--way analysis of variance (ANOVA) model with Bonferroni tests (α=0.05). In the evaluation of the immediate μTBS, only the “adhesive” factor was significant (p <0.05). After 6 months of storage in water, the interaction of the “adhesive and dentinal substrate” factors was significant (p<0.05). The AD in SD (IM 49.0 ± 6.7 MPa) showed a significant decrease in the μTBS after 6 months of storage in water (23.2 ± 7.9 MPa). The SE and AD showed a significant difference (p<0.05) in the SD and DD. The most significant factor for the SD was time, while for the DD, it was the adhesive. The SB in the SD and DD showed no statistically significant differences either immediately or after 6 months (p> 0.05). In conclusion, different levels of dentin depth can affect the bond strength for the same material, and time may influence the degradation of the adhesive system.
Assuntos

Texto completo: Disponível Coleções: Bases de dados internacionais Base de dados: BBO - Odontologia / LILACS Assunto principal: Resistência à Tração / Adesivos Dentinários / Dentina Tipo de estudo: Estudo prognóstico Limite: Humanos Idioma: Português Revista: Braz. dent. sci Assunto da revista: Odontologia / Sa£de Bucal Ano de publicação: 2010 Tipo de documento: Artigo País de afiliação: Brasil Instituição/País de afiliação: Universidade Estadual de Ponta Grossa/BR
Texto completo: Disponível Coleções: Bases de dados internacionais Base de dados: BBO - Odontologia / LILACS Assunto principal: Resistência à Tração / Adesivos Dentinários / Dentina Tipo de estudo: Estudo prognóstico Limite: Humanos Idioma: Português Revista: Braz. dent. sci Assunto da revista: Odontologia / Sa£de Bucal Ano de publicação: 2010 Tipo de documento: Artigo País de afiliação: Brasil Instituição/País de afiliação: Universidade Estadual de Ponta Grossa/BR
...