How erosive drinks and enzyme inhibitors impact bond strength to dentin
MACHADO, Camila Moreira; ZAMUNER, Aline Cristina; MODENA, Karin Cristina da Silva; ISHIKIRIAMA, Sérgio Kiyoshi; WANG, Linda.
Afiliação
  • MACHADO, Camila Moreira; Universidade de São Paulo. Bauru School of Dentistry. Department of Operative Dentistry, Endodontics and Dental Materials. Bauru. BR
  • ZAMUNER, Aline Cristina; Universidade de São Paulo. Bauru School of Dentistry. Department of Operative Dentistry, Endodontics and Dental Materials. Bauru. BR
  • MODENA, Karin Cristina da Silva; Universidade de São Paulo. Bauru School of Dentistry. Department of Operative Dentistry, Endodontics and Dental Materials. Bauru. BR
  • ISHIKIRIAMA, Sérgio Kiyoshi; Universidade de São Paulo. Bauru School of Dentistry. Department of Operative Dentistry, Endodontics and Dental Materials. Bauru. BR
  • WANG, Linda; Universidade de São Paulo. Bauru School of Dentistry. Department of Operative Dentistry, Endodontics and Dental Materials. Bauru. BR
Braz. oral res. (Online) ; 29(1): 1-7, 2015. tab
Artigo em Inglês | LILACS | ID: lil-777199
Biblioteca responsável: BR1.1
ABSTRACT
Concern has been raised about the bonding of restorative procedures to an erosive lesion, given the change in organic and inorganic composition and structure of this substrate. This in vitro study evaluated the effect of erosive drinks and an enzyme inhibitor (2% chlorhexidine digluconate – 2% CHX) on bond strength to dentin. Sixty sound human third molars were selected, and the occlusal enamel was flattened, exposing the dentin surface. The specimens were randomly divided into three groups AS-Artificial saliva (control group), RC- Regular Cola and ZC- Zero Cola. Twenty specimens were immersed in their respective solution for 1 minute, 3 times a day, over the course of 5 days. After acid etching and before bonding with Adper Single Bond 2, half of the samples of each group (n = 10) were treated with 2% CHX, whereas the other half (n = 10) were not, forming the control group (CONV). All the specimens were restored with Filtek Z250 composite resin filled in Tygon tubes (0.48 mm2), yielding six microcylinders for microshear bond strength testing. Three composite resin microcylinders of each specimen were tested after 1 month, and the remaining microcylinders were tested after 6 months. Failure modes were determined using a stereomicroscope (40x). The data were statistically analyzed by three-way ANOVA and Tukey tests (α = 0.05). Overall bonding was reduced after 6 months, regardless of treatment. The 2% CHX enhanced bond strength after 1 month only in the ZC group, and did not enhance bonding performance to demineralized dentin by erosive protocol after 6 months in any group.
Assuntos


Texto completo: Disponível Coleções: Bases de dados internacionais Base de dados: LILACS Assunto principal: Erosão Dentária / Bebidas Gaseificadas / Clorexidina / Dentina / Inibidores Enzimáticos Tipo de estudo: Ensaio clínico controlado / Estudo de avaliação / Guia de prática clínica Limite: Humanos Idioma: Inglês Revista: Braz. oral res. (Online) Assunto da revista: Odontologia Ano de publicação: 2015 Tipo de documento: Artigo / Documento de projeto País de afiliação: Brasil Instituição/País de afiliação: Universidade de São Paulo/BR

Texto completo: Disponível Coleções: Bases de dados internacionais Base de dados: LILACS Assunto principal: Erosão Dentária / Bebidas Gaseificadas / Clorexidina / Dentina / Inibidores Enzimáticos Tipo de estudo: Ensaio clínico controlado / Estudo de avaliação / Guia de prática clínica Limite: Humanos Idioma: Inglês Revista: Braz. oral res. (Online) Assunto da revista: Odontologia Ano de publicação: 2015 Tipo de documento: Artigo / Documento de projeto País de afiliação: Brasil Instituição/País de afiliação: Universidade de São Paulo/BR
...