Your browser doesn't support javascript.
loading
Microshear bond strength evaluation of surface pretreated zirconia ceramics bonded to dentin.
Anand, Shenbagakuttalam; Ebenezar, Ambrose Vedamanickam Rajesh; Anand, Nirupa; Rajkumar, Kothandaraman; Mahalaxmi, Sekar; Srinivasan, Narasimhan.
Afiliação
  • Anand S; Department of Conservative Dentistry and Endodontics, Madha Dental College, Kunrathur, Chennai, India.
  • Ebenezar AVR; Department of Conservative Dentistry and Endodontics, Madha Dental College, Kunrathur, Chennai, India.
  • Anand N; Department of Prosthodontics, Rajah Muthiah Dental College and Hospital, Annamalai University, Chidambaram, India.
  • Rajkumar K; Department of Conservative Dentistry and Endodontics, SRM Dental, Ramapuram, Chennai, India.
  • Mahalaxmi S; Department of Conservative Dentistry and Endodontics, SRM Dental, Ramapuram, Chennai, India.
  • Srinivasan N; Department of Conservative Dentistry and Endodontics, Mahatma Gandhi Post Graduate Institute of Dental Sciences, Pondicherry, India.
Eur J Dent ; 9(2): 224-227, 2015.
Article em En | MEDLINE | ID: mdl-26038654
ABSTRACT

OBJECTIVES:

To comparatively assess the micro shear bond strength (MSBS) of dentin bonded surface pre-treated zirconia ceramics. MATERIALS AND

METHODS:

Zirconia blocks were sectioned into 50 cubical blocks. The blocks were further categorized into five groups (n = 10 each). Group I No treatment was performed on zirconia samples; Group II The zirconia samples were sand-blasted; Group III Group II + etched with 9.8% of hydrofluoric (HF) acid for 60 s; Group IV The sandblasted zirconia samples were selectively infiltrated with low fusing porcelain; and Group V Group IV + etched using 9.8% HF acid gel. The zirconia specimens were then bonded to dentin samples, and the samples were tested for MSBS evaluation using universal testing machine.

RESULTS:

The MSBS of all the four experimental groups shows greater value than group I. Among the experimental groups, group V and group IV do not show any statistical significant difference, whereas the mean MSBS of groups IV and V were statistically greater than group III and group II. However, groups I, II, and III do not show any statistical significant difference in mean MSBS values between them.

CONCLUSION:

Selective infiltration etching of zirconia ceramics provides the highest bond strength with resin cement.