Your browser doesn't support javascript.
loading
Biodegradable sizing agents from soy protein via controlled hydrolysis and dis-entanglement for remediation of textile effluents.
Yang, Maiping; Xu, Helan; Hou, Xiuliang; Zhang, Jie; Yang, Yiqi.
Afiliação
  • Yang M; Key Laboratory of Science & Technology of Eco-Textiles, Ministry of Education, Jiangnan University, 1800 Lihu Road, Wuxi, Jiangsu 214122, China. Electronic address: yangmaiping@sina.com.
  • Xu H; Department of Textiles, Merchandising and Fashion Design, 234, HECO Building, University of Nebraska-Lincoln, Lincoln, NE 68583-0802, United States. Electronic address: hxu14@unl.edu.
  • Hou X; Key Laboratory of Science & Technology of Eco-Textiles, Ministry of Education, Jiangnan University, 1800 Lihu Road, Wuxi, Jiangsu 214122, China. Electronic address: houxiuliang@163.com.
  • Zhang J; Key Laboratory of Science & Technology of Eco-Textiles, Ministry of Education, Jiangnan University, 1800 Lihu Road, Wuxi, Jiangsu 214122, China. Electronic address: 18861823290@163.com.
  • Yang Y; Department of Textiles, Merchandising and Fashion Design, 234, HECO Building, University of Nebraska-Lincoln, Lincoln, NE 68583-0802, United States; Department of Biological Systems Engineering, 234, HECO Building, University of Nebraska-Lincoln, Lincoln, NE 68583-0802, United States; Nebraska Cente
J Environ Manage ; 188: 26-31, 2017 Mar 01.
Article em En | MEDLINE | ID: mdl-27918924
ABSTRACT
Fully biodegradable textile sizes with satisfactory performance properties were developed from soy protein with controlled hydrolysis and dis-entanglement to tackle the intractable environmental issues associated with the non-biodegradable polyvinyl alcohol (PVA) in textile effluents. PVA derived from petroleum is the primary sizing agent due to its excellent sizing performance on polyester-containing yarns, especially in increasingly prevailing high-speed weaving. However, due to the poor biodegradability, PVA causes serious environmental pollution, and thus, should be substituted with more environmentally friendly polymers. Soy protein treated with high amount of triethanolamine was found with acceptable sizing properties. However, triethanolamine is also non-biodegradable and originated from petroleum, therefore, is not an ideal additive. In this research, soy sizes were developed from soy protein treated with glycerol, the biodegradable triol that could also be obtained from soy. The soy sizes had good film properties, adhesion to polyester and abrasion resistance close to PVA, rendering them qualified for sizing applications. Regarding desizing, consumption of water and energy for removal of soy size could be remarkably decreased, comparing to removal of PVA. Moreover, with satisfactory degradability, the wastewater containing soy sizes was readily dischargeable after treated in activated sludge for two days. In summary, the fully biodegradable soy sizes had potential to substitute PVA for sustainable textile processing.
Assuntos
Palavras-chave

Texto completo: 1 Coleções: 01-internacional Base de dados: MEDLINE Assunto principal: Indústria Têxtil / Eliminação de Resíduos Líquidos / Proteínas de Soja Idioma: En Revista: J Environ Manage Ano de publicação: 2017 Tipo de documento: Article

Texto completo: 1 Coleções: 01-internacional Base de dados: MEDLINE Assunto principal: Indústria Têxtil / Eliminação de Resíduos Líquidos / Proteínas de Soja Idioma: En Revista: J Environ Manage Ano de publicação: 2017 Tipo de documento: Article
...