Your browser doesn't support javascript.
loading
Stable Lithium Deposition Enabled by an Acid-Treated g-C3N4 Interface Layer for a Lithium Metal Anode.
Luan, Xiaoyu; Wang, Chenggang; Wang, Chunsheng; Gu, Xin; Yang, Jian; Qian, Yitai.
Afiliação
  • Luan X; Key Laboratory of Colloid and Interface Chemistry, Ministry of Education, School of Chemistry and Chemical Engineering, Shandong University, Jinan 250100, P. R. China.
  • Wang C; Key Laboratory of Colloid and Interface Chemistry, Ministry of Education, School of Chemistry and Chemical Engineering, Shandong University, Jinan 250100, P. R. China.
  • Wang C; Key Laboratory of Colloid and Interface Chemistry, Ministry of Education, School of Chemistry and Chemical Engineering, Shandong University, Jinan 250100, P. R. China.
  • Gu X; Institute of New Energy, College of New Energy, State Key Laboratory of Heavy Oil Processing, China University of Petroleum (East China), Qingdao 266580, P. R. China.
  • Yang J; Key Laboratory of Colloid and Interface Chemistry, Ministry of Education, School of Chemistry and Chemical Engineering, Shandong University, Jinan 250100, P. R. China.
  • Qian Y; Key Laboratory of Colloid and Interface Chemistry, Ministry of Education, School of Chemistry and Chemical Engineering, Shandong University, Jinan 250100, P. R. China.
ACS Appl Mater Interfaces ; 12(9): 11265-11272, 2020 Mar 04.
Article em En | MEDLINE | ID: mdl-32045201
Li metal has been regarded as one of the most promising anode candidates for high-energy rechargeable lithium batteries. Nevertheless, the practical applications of the Li anode have been hampered because of its low Coulombic efficiency and safety hazards. Here, acid-treated g-C3N4 with O- and N-containing groups are coated on Li foil through a facile physical pressing method. The O- and N-containing groups cooperate to rearrange the concentration of Li ions and enhance the Li ion transfer. Hence, the cycle and rate performances of acid-treated g-C3N4-coated Li electrodes are greatly improved in symmetric cells, which show cycling stability over 400 h at 1 mA cm-2 in ester-based electrolytes and over 2100 h in ether-based electrolytes. As for the Li//LiFePO4 full cells, there is a high capacity retention of 80% over 400 cycles at 1 C. The full cells of Li//S in ether-based electrolytes also exhibit a capacity of 520 mA h g-1 after 400 cycles at 1 C.