Sustainably recycling spent lithium-ion batteries to prepare magnetically separable cobalt ferrite for catalytic degradation of bisphenol A via peroxymonosulfate activation.
Liang, Jianxing; Xue, Yixin; Gu, Jia-Nan; Li, Jingdong; Shi, Feng; Guo, Xin; Guo, Mingming; Min, Xin; Li, Kan; Sun, Tonghua; Jia, Jinping.
Afiliação
  • Liang J; School of Environmental Science and Engineering, Shanghai Jiao Tong University, 800 Dong Chuan Road, Shanghai 200240, PR China. Electronic address: k.s.leung@sjtu.edu.cn.
  • Xue Y; School of Environmental Science and Engineering, Shanghai Jiao Tong University, 800 Dong Chuan Road, Shanghai 200240, PR China. Electronic address: xueyixin@sjtu.edu.cn.
  • Gu JN; School of Environmental Science and Engineering, Shanghai Jiao Tong University, 800 Dong Chuan Road, Shanghai 200240, PR China. Electronic address: gujianan96@sjtu.edu.cn.
  • Li J; School of Environmental Science and Engineering, Shanghai Jiao Tong University, 800 Dong Chuan Road, Shanghai 200240, PR China. Electronic address: sjtulijingdong@sjtu.edu.cn.
  • Shi F; School of Environmental Science and Engineering, Shanghai Jiao Tong University, 800 Dong Chuan Road, Shanghai 200240, PR China. Electronic address: shifeng51@sjtu.edu.cn.
  • Guo X; School of Environmental Science and Engineering, Shanghai Jiao Tong University, 800 Dong Chuan Road, Shanghai 200240, PR China. Electronic address: 13641533909@139.com.
  • Guo M; School of Environmental Science and Engineering, Shanghai Jiao Tong University, 800 Dong Chuan Road, Shanghai 200240, PR China; Shanghai Engineering Research Center of Solid Waste Treatment and Resource Recovery, Shanghai 200240, PR China. Electronic address: mingmingguo@sjtu.edu.cn.
  • Min X; School of Environmental Science and Engineering, Shanghai Jiao Tong University, 800 Dong Chuan Road, Shanghai 200240, PR China. Electronic address: sjtuminxin@sjtu.edu.cn.
  • Li K; School of Environmental Science and Engineering, Shanghai Jiao Tong University, 800 Dong Chuan Road, Shanghai 200240, PR China; Shanghai Institute of Pollution Control and Ecological Security, Shanghai 200092, PR China. Electronic address: likan@sjtu.edu.cn.
  • Sun T; School of Environmental Science and Engineering, Shanghai Jiao Tong University, 800 Dong Chuan Road, Shanghai 200240, PR China; Shanghai Engineering Research Center of Solid Waste Treatment and Resource Recovery, Shanghai 200240, PR China. Electronic address: sunth@sjtu.edu.cn.
  • Jia J; School of Environmental Science and Engineering, Shanghai Jiao Tong University, 800 Dong Chuan Road, Shanghai 200240, PR China; Shanghai Institute of Pollution Control and Ecological Security, Shanghai 200092, PR China. Electronic address: jpjia@sjtu.edu.cn.
J Hazard Mater ; 427: 127910, 2022 Apr 05.
Article em En | MEDLINE | ID: mdl-34863568

Texto completo: 1 Coleções: 01-internacional Base de dados: MEDLINE Idioma: En Revista: J Hazard Mater Assunto da revista: SAUDE AMBIENTAL Ano de publicação: 2022 Tipo de documento: Article País de publicação: Holanda

Texto completo: 1 Coleções: 01-internacional Base de dados: MEDLINE Idioma: En Revista: J Hazard Mater Assunto da revista: SAUDE AMBIENTAL Ano de publicação: 2022 Tipo de documento: Article País de publicação: Holanda