Your browser doesn't support javascript.
loading
The Effect of Topical Agents on the Tensile Strength of Absorbable and Non-absorbable Suture Materials-An in Vitro Study.
Alnaqi, Amar; Burhamah, Waleed; Al-Sultan, Ahmad T; Taqi, Esmaeel.
Afiliação
  • Alnaqi A; Faculty of Medicine, Department of Surgery, Kuwait University, Kuwait City, Kuwait. Dralnaqi@gmail.com.
  • Burhamah W; Department of Pediatric Surgery, Ibn Sina Hospital, Sabah Medical Region, Kuwait City, Kuwait. Dralnaqi@gmail.com.
  • Al-Sultan AT; Royal College of Surgeons in Ireland, Dublin, Ireland.
  • Taqi E; Department of Community Medicine and Behavioral Sciences College of Medicine, Kuwait University, Kuwait City, Kuwait.
World J Surg ; 47(2): 448-454, 2023 02.
Article em En | MEDLINE | ID: mdl-36316513
INTRODUCTION: Topical agents are sometimes applied to surgical wounds after closure; these may include antiseptics or antibiotics. Minimal research has been undertaken to investigate the effect of topical regimens on the tensile strength of suture materials. AIM: To investigate the effect of four commonly used wound care regimens on the tensile strength of suture materials. METHODS: The failure load of 9 different suture materials was tested using the Instron Electroplus E3000 tensile testing machine (Instron Corporation, Norwood, Massachusetts). Tensile strength was represented as the failure load, measured in Newtons (N), and defined as the maximal load that could be applied across the suture prior to failure. Each suture was tested dry and after immersion in one of 4 products for 7 days and tested on day 7. The immersion agents tested were: sodium chloride 0.9%, MicroSafe® (Sonoma Pharmaceuticals, Petaluma, CA), Aqueous Povidone-iodine 10% solution (Betadine-Mundipharma), and Fucidin ointment. RESULTS: Sodium chloride 0.9%, MicroSafe®, Aqueous Povidone-iodine 10%, and Fucidin seem to increase the failure load of most absorbable and non-absorbable sutures. However, the failure load of Polyglactin 910 suture (Surgilactin, coated, violet-Ethicon) is reduced by long-term exposure to either sodium chloride 0.9% or MicroSafe®, while the failure load of the Polydioxanone suture (PDS Plus-Ethicon) is reduced by long-term exposure to MicroSafe® only. CONCLUSION: In our experiment, the commonly used wound care products have been shown to alter the tensile strength of suture materials. Further human studies are required to ascertain the clinical validity and applicability of our findings.