Your browser doesn't support javascript.
loading
Effects of alpha-tocopherol antioxidant on fracture strength and adhesion of endodontically treated teeth restored after dental bleaching.
Marcomini, Natália; Albaricci, Maria Carolina da Costa; Costa, Joatan Lucas de Sousa Gomes; Besegato, João Felipe; Godoy, Eduardo Fernández; Dantas, Andréa Abi Rached; Kuga, Milton Carlos.
Afiliação
  • Marcomini N; Department of Restorative Dentistry, School of Dentistry, Araraquara, São Paulo State University - UNESP, Araraquara, São Paulo, Brazil.
  • Albaricci MCDC; Department of Restorative Dentistry, School of Dentistry, Araraquara, São Paulo State University - UNESP, Araraquara, São Paulo, Brazil.
  • Costa JLSG; Department of Restorative Dentistry, School of Dentistry, Araraquara, São Paulo State University - UNESP, Araraquara, São Paulo, Brazil.
  • Besegato JF; Department of Restorative Dentistry, School of Dentistry, Federal University of Minas Gerais - UFMG, Belo Horizonte, Minas Gerais, Brazil.
  • Godoy EF; School of Dentistry, Federal University of Mato Grosso do Sul - UFMS, Campo Grande, Mato Grosso do Sul, Brazil.
  • Dantas AAR; Instituto de Ciencias Biomédicas, Universidad Autónoma de Chile, Santiago, Chile.
  • Kuga MC; Department of Restorative Dentistry, School of Dentistry, Araraquara, São Paulo State University - UNESP, Araraquara, São Paulo, Brazil.
Eur J Oral Sci ; 132(1): e12965, 2024 Feb.
Article em En | MEDLINE | ID: mdl-38115770
ABSTRACT
This study evaluated the effect of different concentrations of alpha-tocopherol in gel form on fracture strength, hybrid layer formation, and microtensile bond strength of endodontically treated teeth bleached with 40% hydrogen peroxide (H2 O2 ). Sixty bovine incisors were randomized into one of six groups (n = 10 incisors per group) defined by the interventions carried out after endodontic treatment. In the control group, no additional intervention was carried out, while all teeth in the five intervention groups were bleached with 40% H2 O2 and subsequently treated with alpha-tocopherol at concentrations of 15% (15AT), 20% (20AT), or 25% (25AT), with 10% sodium ascorbate (10SA), or with nothing (40HP). Fracture strength was evaluated in a mechanical testing machine, hybrid layer formation was assessed using scanning electron microscopy, and bond strength was determined using microtensile bond-strength testing. Data were analyzed using Kruskal-Wallis and Dunn's tests. No statistically significant difference regarding fracture strength was observed among groups. Hybrid layer formation was greater in the 15AT group than in groups 40HP and 10SA. Teeth in groups 15AT, 20AT, and 25AT demonstrated higher bond strength than teeth in groups 40HP and 10SA. Alpha-tocopherol, preferably at 15%, effectively reverses the deleterious effects, of bleaching, on hybrid layer formation and bond strength to dentin.
Assuntos
Palavras-chave

Texto completo: 1 Coleções: 01-internacional Base de dados: MEDLINE Assunto principal: Clareamento Dental / Colagem Dentária / Dente não Vital Limite: Animals Idioma: En Revista: Eur J Oral Sci Assunto da revista: ODONTOLOGIA Ano de publicação: 2024 Tipo de documento: Article País de afiliação: Brasil

Texto completo: 1 Coleções: 01-internacional Base de dados: MEDLINE Assunto principal: Clareamento Dental / Colagem Dentária / Dente não Vital Limite: Animals Idioma: En Revista: Eur J Oral Sci Assunto da revista: ODONTOLOGIA Ano de publicação: 2024 Tipo de documento: Article País de afiliação: Brasil