Your browser doesn't support javascript.
loading
Stereo-complex polylactide composite aerogel for crude oil adsorption.
Zhang, Weijian; Zhang, Mingtao; Chen, Qiang; Liu, Xianhu.
Afiliação
  • Zhang W; State Key Laboratory of Solidification Processing, Northwestern Polytechnical University, Xi'an 710072, China; State Key Laboratory of Structural Analysis, Optimization and CAE Software for Industrial Equipment, National Engineering Research Center for Advanced Polymer Processing Technology, Zhengzh
  • Zhang M; State Key Laboratory of Structural Analysis, Optimization and CAE Software for Industrial Equipment, National Engineering Research Center for Advanced Polymer Processing Technology, Zhengzhou University, Zhengzhou 450002, China. Electronic address: 12329032@zju.edu.cn.
  • Chen Q; State Key Laboratory of Solidification Processing, Northwestern Polytechnical University, Xi'an 710072, China. Electronic address: qiang.chen@nwpu.edu.cn.
  • Liu X; State Key Laboratory of Structural Analysis, Optimization and CAE Software for Industrial Equipment, National Engineering Research Center for Advanced Polymer Processing Technology, Zhengzhou University, Zhengzhou 450002, China. Electronic address: xianhu.liu@zzu.edu.cn.
Int J Biol Macromol ; 263(Pt 1): 130283, 2024 Apr.
Article em En | MEDLINE | ID: mdl-38378113
ABSTRACT
Adsorption materials are a cost-effective and simple method for oil spill remediation, but their efficiency is limited by high crude oil viscosity. Additionally, non-degradable materials pose another risk of secondary pollution, such as microplastic debris. Here, an environmentally-friendly stereo-complex polylactide composite (SCC) aerogel were developed via water-assisted thermally induced phase separation. The SCC with 3 wt% carbon nanotubes had a hierarchical structure of micro/nanoscale pores and high content of stereo-complex crystallites (35.7 %). Along with the excellent water repellency (water contact angle 157°), SCC aerogel was 2.7 times as resistant to hydrolysis than poly(l-lactide) aerogel (Ph = 13, 37 °C). Additionally, a maximum absorption capacity of 41.2 g g-1 and over 97 % oil/water separation efficiency after 10 cycles were obtained in low viscosity conditions; while in high viscosity conditions, it displayed excellent photothermal performance, reaching a surface temperature of 85 °C under 1 sunlight, reducing crude oil absorption time from 42 min to 60 s (97.6 %-time savings). Moreover, it facilitated continuous crude oil spill recovery under sunlight with an adsorption rate of 3.3 × 104 kg m-3 h-1. The SCC aerogel presents a potential route for utilizing solar energy in crude oil adsorption applications without additional environmental burden.
Assuntos
Palavras-chave

Texto completo: 1 Coleções: 01-internacional Base de dados: MEDLINE Assunto principal: Poliésteres / Petróleo / Nanotubos de Carbono Idioma: En Revista: Int J Biol Macromol Ano de publicação: 2024 Tipo de documento: Article País de publicação: Holanda

Texto completo: 1 Coleções: 01-internacional Base de dados: MEDLINE Assunto principal: Poliésteres / Petróleo / Nanotubos de Carbono Idioma: En Revista: Int J Biol Macromol Ano de publicação: 2024 Tipo de documento: Article País de publicação: Holanda